| 高锰奥氏体钢中锰的异常偏析 |
| 葛云龙;柴寿森 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| ABNORMAL SEGREGATION OF Mn IN AN AUSTENITIC HIGH-Mn STEEL |
| Ge Yunlong and Chai Shousen (Institute of Metal Research; Academia Sinica) |
引用本文:
葛云龙;柴寿森. 高锰奥氏体钢中锰的异常偏析[J]. 金属学报, 1981, 17(6): 687-689.
,
.
ABNORMAL SEGREGATION OF Mn IN AN AUSTENITIC HIGH-Mn STEEL[J]. Acta Metall Sin, 1981, 17(6): 687-689.
[1] 柴寿森,葛云龙,钢铁,16(1981) ,№.8,46. [2] Yu, J. and McMahon, C. J., Jr., Metall. Trans., 11A (1980) , 291. [3] Joshi, A., Palmberg, P. W, and Stein, D. F., Metall. Trans., 6 (1975) , 2160. [4] Olefjord, I., Int. Met. Rev., 23 (1978) , 149. [5] Guttmann, M., Surf. Soi., 53 (1975) , 213 |
|