| 模糊对称群与非晶态结构的短程序 |
| 郑兆勃 |
| 美国肯塔基州路易维尔大学物理系;中国科学技术大学物理系赴美进修教师 |
|
| FUZZY SYMMETRIC GROUP AND SHORT-RANGE ORDER IN THE STRUCTURE OF AMORPHOUS SOLIDS |
| Zheng Zhaobo (University of Science and Technology of China; recently engaged in advanced studies at Department of Physics; University of Louisville; Kentucky; U. S. A.; when the reseaech was carried out) |
引用本文:
郑兆勃. 模糊对称群与非晶态结构的短程序[J]. 金属学报, 1981, 17(6): 643-651.
.
FUZZY SYMMETRIC GROUP AND SHORT-RANGE ORDER IN THE STRUCTURE OF AMORPHOUS SOLIDS[J]. Acta Metall Sin, 1981, 17(6): 643-651.
[1] Finney, J. L., Nature, 266 (1977) , 309. [2] 干福熹,科学通报,2(1963) ,18. [3] 干福熹,硅酸盐学报,7(1979) ,150. [4] 干福熹,中国科学,(1974) ,№.4,351. [5] 早稻田嘉夫,固体物理,12(1977) ,181. [6] Bernal, J. D., Nature, 183 (1959) , 141. [7] Kanfmann, A., Introduction to the Theory of Fuzzy Subsets, Vol. 1, Academic Press, New York, 1975, p. 3. [8] Connell, G. A. N. and Lucovsky, G., Non-Cryst. Solids, 31 (1978) , 123.` |
|