| 用双试样求材料的J_(IC) |
| 魏文光;王广生;张中林;陆丁昌 |
| 长城钢厂;长城钢厂;长城钢厂;长城钢厂 |
|
| DOUBLE-SPECIMEN METHOD FOR J_(IC) TSETING |
| by Wei Wenguang; Wang Guangsheng; Zhang Zhonglin and Lu Dingchang(Changcheng Steel Works) |
引用本文:
魏文光;王广生;张中林;陆丁昌. 用双试样求材料的J_(IC)[J]. 金属学报, 1981, 17(4): 478-483.
,
,
,
.
DOUBLE-SPECIMEN METHOD FOR J_(IC) TSETING[J]. Acta Metall Sin, 1981, 17(4): 478-483.
[1] 陈篪等,金属断裂研究文集,冶金工业出版社,1978,p.93. [2] 日本机械学会論文集,№ 358,通常总会講演会,第42期,1976. |
|