| 稀土硅铁合金粉化原因的探讨 |
| 高怀荪;蒋景凯 |
| 包头冶金研究所;包头冶金研究所 |
|
| ON THE SELF-POWDERING OF RE-Si-Fe ALLOY |
| by Gao Huaisun and Jiang Jingkai (Baotou Institute of Metallurgy Research) |
引用本文:
高怀荪;蒋景凯. 稀土硅铁合金粉化原因的探讨[J]. 金属学报, 1981, 17(4): 484-503.
,
.
ON THE SELF-POWDERING OF RE-Si-Fe ALLOY[J]. Acta Metall Sin, 1981, 17(4): 484-503.
[1] 内部资料. [2] U. S. Pat. 3,440,041, (1977) . [3] 奥田,钦之助,日本特許出愿公開 昭51-101717,9. 8. [4] Ono, S., Nomuka, K. and Hayakawa, H., J. Less-Common Met., 38 (1974) , 119. |
|