| 显微硬度的常量和相对比较测试方法 |
| 赵所琛;桂运平 |
| 上海第三钢铁厂;上海原子核研究所 |
|
| ON THE TESTING METHODS OF MICROHARDNESS BY DETERMINATION OF CONSTANT & RELATIVE COMPARISON |
| Zhao Suoshen;Gui Yunping Shanghai № 3 Steel Works Shanghai Institute of Atomic Nucleus |
引用本文:
赵所琛;桂运平. 显微硬度的常量和相对比较测试方法[J]. 金属学报, 1979, 15(1): 167-172.
,
.
ON THE TESTING METHODS OF MICROHARDNESS BY DETERMINATION OF CONSTANT & RELATIVE COMPARISON[J]. Acta Metall Sin, 1979, 15(1): 167-172.
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|