| 非晶态的形成 |
| 郑兆勃 |
| 中国科学技术大学物理系 |
|
| ON THE FORMATION OF AMORPHOUS SOLIDS |
| Zheng Zhaobo Dept;of Physics; University of Science and Technology of China |
引用本文:
郑兆勃. 非晶态的形成[J]. 金属学报, 1979, 15(1): 155-166.
.
ON THE FORMATION OF AMORPHOUS SOLIDS[J]. Acta Metall Sin, 1979, 15(1): 155-166.
[1] Vogel, W., J. Non-Cryst. Solids, 25 (1977) , 179. [2] Cohen, M. H. and Turnbull, D., J. Chem. Phys., 31 (1959) , 1164. [3] Turnbull, D. and Cohen, M. H., J. Chem. Phys., 34 (1961) , 120. [4] Turnbull, D. and Cohen, M. H., J. Chem. Phys., 52 (1970) , 3038. [5] Gibbs, J. H. and DiMarzio, E. A., J. Chem. Phys., 28 (1958) , 373. [6] Adam, G. and Gibbs, J. H., J. Chem Phys., 43 (1965) , 139. [7] Gutzow, I., in "Amorphous Materials", Proc. Ⅲ Int. Conf. Non-Crystalline Solids, 1972, Wiley, London, p. 159. [8] Uhlmann, D. R., J. Non-Cryst. Solids. 25 (1977) , 42. [9] Turnbull, D., Contemp. Phys., 10 (1969) , 473. [10] Hruby, A., Czech. J. Phys., B22 (1972) , 1187. [11] Vreeswijk. J. C. A. et al., J. Non-Cryst. Solids, 16 (1974) , 15. [12] Gutzow. I. and Iavvamov, J. Non-Cryst. Solids. 16 (1974) , 128. [13] Turnbull, D. and Cohen, M. H, J. Chem. Phys., 29 (1958) , 1049. [14] Duwez, P., Willens, R. H. and Klement, W., J. Appl. Phys.. 31 (1960) , 1136. [15] Sarjeant. P. T. and Roy. R.. Mater. Res. Bull., 3 (1968) . 265. [16] Uhlmann. D. R., J. Non-Cryst. Solids, 17 (1975) . 266. [17] Onorato. P. I. K. and Uhlmann, D. R., J. Non-Cryst. Solids, 7 (1972) , 337. [18] Davies, H. A., J. Non-Cryst. Solids, 17 (1975) , 266. [19] Clsvaguera, N., J. Non-Cryst. Solids, 22 (1976) , 23. [20] Tauc, J., Amorphous and Liquid Semiconductors, Plenum, New York. 1974, pp. 1-39. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|