摘要: 本文导出了体心立方和面心立方挛晶复合倒易点阵的六角单胞。利用这两种模型可以形象地说明立方挛晶电子衍射谱的花样特点,从而能进一步简化其衍射谱的计算和标定过程。
Abstract:Hexagonal unit cells of composite reciprocal lattice have been derived for bcc as well as for fcc twin crystals, with these models, the characteristics of electron diffraction patterns of twinning in cubic systems can be figuratively described, thus simplifying the calculating and indexing processes of these patterns.
收稿日期: 1978-04-18     
[1] Pashley, D. W. and Stowell, M. J., Phil Mag., 8 (1963) , 1605. Hirsch. P. B. et al., Electron Microscopy of Thin Crystals, Butterworths, London, 1975, p. 145,
[2] Edington, J. W., Electron Diffraction in the Electron Microscope, Philips, London and Basingstoke, 1975, p. 47.
[3] 桶谷繁雄,電子線回折金属碳化物研究,東京,1971,p.69.
[4] #12
[5] Kelly, P. M., Trans. AIME, 233 (1965) , 264.
[6] Andrews, K. W. et al, Interpretation of Electron Diffraction Patterns, Hilger, London, 1971, p. 53.
[7] 陈乾惕,金属学报,14(1978) ,428.
[8] 电子衍射,中国科学院金属研究所技术资料,1976.
No related articles found!