| 用多次冲击法测定金属断裂韧性 |
| 杨峥 |
| 西北工业大学 |
|
| FRACTURE TOUGHNESS TEST BY IMPACT-FATIGUE METHOD |
| Yang Zheng (North-West Engineering Institute) |
引用本文:
杨峥. 用多次冲击法测定金属断裂韧性[J]. 金属学报, 1978, 14(4): 409-468.
.
FRACTURE TOUGHNESS TEST BY IMPACT-FATIGUE METHOD[J]. Acta Metall Sin, 1978, 14(4): 409-468.
[1] 陈篪,力学,1974,№ 4,121. [2] 北京钢铁研究院断裂韧性研究组,金属学报,13(1977) ,214. [3] Turner, C.E., Impact Testing of Metals, Amer. Soc. Test. Mater., Spec. Tech. Publ. № 466, (1970) , p. 93.\ |
|