| 中碳镍铬钼钢中夹杂物和韧窝断口形貌关系的初步观察 |
| 赵坚 |
|
| ON THE RELATION BETWEEN INCLUSIONS AND MORPHOLOGY OF DIMPLE FRACTURES IN CERTAIN STEELS |
| Zhao Jian |
引用本文:
赵坚. 中碳镍铬钼钢中夹杂物和韧窝断口形貌关系的初步观察[J]. 金属学报, 1978, 14(3): 316-348.
.
ON THE RELATION BETWEEN INCLUSIONS AND MORPHOLOGY OF DIMPLE FRACTURES IN CERTAIN STEELS[J]. Acta Metall Sin, 1978, 14(3): 316-348.
|