| 残余元素的表面富集与晶界氧化——关于低碳钢热脆机理的讨论 |
| 刘富有 |
| 昆明钢铁厂中心试验室 |
|
| SURFACE ENRICHMENT OF RESIDUAL ELEMENTS AND OXIDATION OF THE AUSTENITE GRAIN BOUNDARIES——A Study on the Hot Shortness Mechanism of Mild Steel |
| Liu Fu-you(Central Laboratory of Kunming Iron and Steer Works) |
引用本文:
刘富有. 残余元素的表面富集与晶界氧化——关于低碳钢热脆机理的讨论[J]. 金属学报, 1978, 14(3): 310-347.
.
SURFACE ENRICHMENT OF RESIDUAL ELEMENTS AND OXIDATION OF THE AUSTENITE GRAIN BOUNDARIES——A Study on the Hot Shortness Mechanism of Mild Steel[J]. Acta Metall Sin, 1978, 14(3): 310-347.
[1] Menter, J. W., J. Iron Steel Inst., 209 (1971) , 249. [2] Melford, D. A., J. Iron Steel Inst., 200 (1962) , 290. [3] Melford, D. A., J. Iron Steel Inst., 204 (1966) , 495. [4] Salter, W. J. M., J. Iron Steel Inst., 204 (1966) , 478. [5] Salter, W. J. M., J. Iron Steel Inst., 205 (1967) , 1156. [6] Nicholson, A. and Murray, J. D., J. Iron, Steel Inst., 203 (1965) , 1007. [7] 田上豊助,河合忠二,铁鋼,52(1966) ,624. [8] Cox, A. R. and Winn, J. M., J. Iron Steel Inst., 203 (1965) , 175. [9] Stephenson, E. T., J. Metals, 26 (1974) , 48. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|