|
|
|
| 铅、锡、镁在液态镓汞间的分配 |
| 李爱珍;邹元爔 |
| 中国科学院冶金研究所;中国科学院冶金研究所 |
|
| DISTRIBUTION OF LEAD, TIN AND MAGNESIUM BETWEEN LIQUID GALLIUM AND MERCURY |
| LI AI-CHEN;CHOU YUAN-HSI Institute of Metallurgy; Academia Sinica |
引用本文:
李爱珍;邹元爔. 铅、锡、镁在液态镓汞间的分配[J]. 金属学报, 1965, 8(2): 193-196.
,
.
DISTRIBUTION OF LEAD, TIN AND MAGNESIUM BETWEEN LIQUID GALLIUM AND MERCURY[J]. Acta Metall Sin, 1965, 8(2): 193-196.
[1] 刘民治:物理学报,1959,15,389。 [2] Pierre De La Breteque: Preparation of Ⅲ--Ⅴ Compounds, (Reinhold, 1962) , p. 68. [3] Plust, H. G.: Ger. (West) Patent, No. 1,002,012, 1956. [4] Spicer, W. M., Bartholomay, H. W.: J. Am. Chem. Soc., 1951, 73, 868. [5] #12 [6] Rand, M. H., Kubaschewski, O.: The Thermochemical Properties of Uranium Compounds, (Oliver & Boyd, 1963) , p. 52. [7] Kubaschewski, O., Catterall, J. A.: Thermochemical data of Alloys, (Pergamon, 1956) , p. 101, 104. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|