金属学报  1965, Vol. 8 Issue (2): 197-203    
  论文 本期目录 | 过刊浏览 |
碳、氧在纯铁浮区熔化过程中的行为
王伟杰
中国科学院冶金研究所
BEHAVIOR OF CARBON AND OXYGEN IN FLOATING-ZONE MELTING OF PURE IRON
WANG WEI-CHIEH Institute of Metallurgy; Academia Sinica
引用本文:

王伟杰. 碳、氧在纯铁浮区熔化过程中的行为[J]. 金属学报, 1965, 8(2): 197-203.
. BEHAVIOR OF CARBON AND OXYGEN IN FLOATING-ZONE MELTING OF PURE IRON[J]. Acta Metall Sin, 1965, 8(2): 197-203.

全文: PDF(926 KB)  
摘要: 报导了纯铁浮区熔化过程中杂质碳、氧的行为。电解铁经真空感应熔炼和真空铸锭后,制成直径为10毫米的试样。当区域熔化时,熔区下的试样以3.5—22转/分的速度旋转,而熔区自下而上地以1—2毫米/分的速度沿试样移动。试样经过11次区域熔化。 根据碳的分布系数的测定和区熔前后试样中夹杂物的金相鉴定,讨论了区域熔化法去除铁中碳、氧杂质的可能性。
Abstract:Vacuum melted and cast electrolytic iron bar, 10 mm in diameter, has been refinedby the floating-zone technique for eleven passes in an atmosphere of hydrogen. Thetravel rate of the zone was 1-2 mm/min and the lower chuck was rotated at a speed of3.5-22 rpm. On the basis of the measured distribution coefficient of carbon and metallographicexamination of the non-metallic inclusions the possibility of removing carbon and oxygenfrom iron by floating-zone melting is discussed.
收稿日期: 1965-02-18     
[1] Keck, P. H., Golay, M. J. E.: Phys. Rev., 1953, 89, 1297.
[2] Cunnell, F. A., Wickham, R.: J. Sci. Instr., 1960, 37, 410.
[3] Bardsley, W.: Res. Appl. Ind., 1959, 12, 183.
[4] Oliver, B. F., Shafer. A. J. Trans. AIME. 1960. 218. 194.
[5] 京谷益次、绕木路南、西川和幸:日本金属学会志,1960,24,391.
[6] Smith, R. L., Rutherford, J. L.: Trans. AIME, 1957, 209, 478.
[7] Fischer, W. A., Spitzer, H., Hishinuma, M.: Arch. Eisenhuttenw., 1960, 365.
[8] Hillmann, H., Mager, A.: Z. Metallk., 1960, 51. 663.
[9] 中村卫:日本金属学会志,1962,26,391。
[10] Williams, W. M., Craig, G. B., Winegard, W. C.: Can. Mining Met. Bull., 1962, 55, 35.
[11] Simonsen, E. B.: J. Iron Steel Inst. (London). 1962, 200, 193.
[12] 大岡耕之、三村宏、矢野清之助等:日本金属学会志,1963,27,342.
[13] 何焕南、严荣华、俞柏华:改良低压燃烧法测定金属中微量碳,待发表.
[14] Chipman, J.: Basic Open Hearth Steelmaking, 2nd ed., (AIME, 1951) , p. 632.
[15] Hayes, A., Chipman, J.: Trans. AIME 1939, 135, 85.
[16] Hansen, M.: Constitution of Binary Alloys, 2nd ed., (McGraw-Hill, 1958) .
[17] Tiller, W. A.: J. Iron Steel Inst. (London), 1959, 192, 338.
[18] #12
[19] Pfann, W. G.: Zone Melting, (Wiley, 1958) , p. 16.
[20] Darken, L. S.: Basic Open Hearth Steelmaking, 2nd ed., (AIME, 1951) , p. 610.
[21] Seybolt, A. U.: J. Metals, 1954, 6, 979.
[22] Pfann, W. G.: Science, 1962, 135, 1101.
[23] Wroughton, D. M., Okress, E. C., Brace, P. H. et al.: J. Electrochem. Soc., 1952, 99, 205.
No related articles found!