| 溶体的次正规模型对二元平衡图热力学分析的运用 |
| 田德诚;朱锡熊 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| APPLICATION OF THE SUB-REGULAR SOLUTION MODEL TO THE THERMODYNAMICAL ANALYSIS OF BlNARY EQUILIBRIUM DIAGRAMS |
| T'IEN TEH-CHENG;CHU HSI-HSIUNG Institute of Metal Research; Academia Sinica |
引用本文:
田德诚;朱锡熊. 溶体的次正规模型对二元平衡图热力学分析的运用[J]. 金属学报, 1965, 8(1): 38-50.
,
.
APPLICATION OF THE SUB-REGULAR SOLUTION MODEL TO THE THERMODYNAMICAL ANALYSIS OF BlNARY EQUILIBRIUM DIAGRAMS[J]. Acta Metall Sin, 1965, 8(1): 38-50.
[1] Hildebrand, J. H.: J. Am. Chem. Soc., 1929, 51, 66. 参阅Hildebrand, J. H., Scott, R. L.: The Solubility of Nonelectrolytes, 3rd ed., (Reinhold, 1950) , p. 46. [2] Becker, R.: Z. Metallk., 1937, 29, 245. [3] #12 [4] #12 [5] #12 [6] Hardy, H. K.: Acta Met., 1953, 1, 202. [7] #12 [8] Guggenheim, E. A.: Trans. Faraday Soc., 1937, 33, 151. [9] Lawson, A. W.: Thermodynamics in Physical Metallurgy, (ASM. 1950) , p. 85. [10] Hansen, M., Anderko, K.: Constitution of Binary Alloys, 2nd ed., (McGraw-Hill, 1958) . [11] Kelley, K. K.: Contributions to the Data on Theoretical Metallurgy XIII. High Temperature Heat-Content, Heat-Capacity, and Entropy Data for the Elements and Inorganic Compounds, (U. S. Bureau of Mines, Bull. No. 584, 1960) . [12] Kubaschewski, O., Evans, E. LL.: Metallurgical Thermochemistry, (Pergamon, 1958) , p. 344. [13] Vieland, L. J.: Actd Met., 1963, 11, 137. [14] Liu, T S. (刘天锡), Peretti, E. A.: Trans. Am. Soc. Metals, 1952, 44, 539. [15] #12 [16] Schottky, W. F., Bever, M. B.: Acta Met., 1958, 6, 320. [17] Darken, L. S., Gurry, R. W.: Physical Chemistry of Metals, (Department of Metallurgy Massachusetts Institute Technology, 1953) , p. 235--282. [18] Lumsden, J.: Thermodynamics of Alloys, (Inst. Metals, 1952) , p. 203. [19] Nachtrieb, N. H., Clement, N.: J. Phys. Chem., 1958, 62, 876. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|