| 金属学报 DOI: 10.11900/0412.1961.2026.00063 |
|
|
|
| 基于响应面法的热等静压近净成形Ti-5Al-2.5Sn超低间隙元素合金的工艺参数优化 |
| 李若辰1,2 卢正冠2 窦 唯3 田晓生2 崔潇潇2 徐 磊2 |
1 中国科学技术大学 材料科学与工程学院 沈阳 110016
2 中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016
3 北京航天动力研究所 北京 100076
|
|
| MethodologyProcess Parameter
Optimization for Hot Isostatic Pressing of Ti–5Al–2.5Sn Extra Low Interstitial
Alloy by Response Surface Methodology |
| LI Ruochen 1, 2,
LU Zhengguan 2, DOU Wei 3, TIAN Xiaosheng 2,
CUI Xiaoxiao 2, XU Lei 2 |
1 School
of Materials Science and Engineering, University of Science and Technology of
China, Shenyang 110016, China
2
Shi-changxu Innovation Center for Advanced Materials, Institute of Metal
Research, Chinese Academy of Sciences, Shenyang 110016, China
3 Beijing
Aerospace Propulsion Institute, Beijing 100076, China
|
引用本文:
李若辰, 卢正冠, 窦唯, 田晓生, 崔潇潇, 徐磊. 基于响应面法的热等静压近净成形Ti-5Al-2.5Sn超低间隙元素合金的工艺参数优化[J]. 金属学报, DOI: 10.11900/0412.1961.2026.00063.
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|