不锈钢网上水热制备NiCo2O4/MoS2纳米复合结构及其在电解水制氢中的应用 |
李丹1,2, 李杨1,2, 陈荣生1,2, 倪红卫1,2() |
1 武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室 武汉 430081 2 武汉科技大学省部共建耐火材料与冶金国家重点实验室 武汉 430081 |
|
Direct Synthesis of NiCo2O4 Nanoneedles and MoS2 Nanoflakes Grown on 316L Stainless Steel Meshes by Two Step Hydrothermal Method for HER |
Dan LI1,2, Yang LI1,2, Rongsheng CHEN1,2, Hongwei NI1,2() |
1 Key Laboratory for Ferrous Metallurgy and Resources Utilization of Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081, China 2 State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081, China |
引用本文:
李丹, 李杨, 陈荣生, 倪红卫. 不锈钢网上水热制备NiCo2O4/MoS2纳米复合结构及其在电解水制氢中的应用[J]. 金属学报, 2018, 54(8): 1179-1186.
Dan LI,
Yang LI,
Rongsheng CHEN,
Hongwei NI.
Direct Synthesis of NiCo2O4 Nanoneedles and MoS2 Nanoflakes Grown on 316L Stainless Steel Meshes by Two Step Hydrothermal Method for HER[J]. Acta Metall Sin, 2018, 54(8): 1179-1186.
[1] | Lewis N S, Nocera D G.Powering the planet: Phemical challenges in solar energy utilization[J]. Proc. Natl. Acad. Sci. USA, 2006, 103: 15729 | [2] | Xiang Z C, Zhang Z, Xu X J, et al.MoS2 nanosheets array on carbon cloth as a 3D electrode for highly efficient electrochemical hydrogen evolution[J]. Carbon, 2016, 98: 84 | [3] | Chu S, Majumdar A.Opportunities and challenges for a sustainable energy future[J]. Nature, 2012, 488: 294 | [4] | Deng Z H, Li L, Ding W, et al.Synthesized ultrathin MoS2 nanosheets perpendicular to graphene for catalysis of hydrogen evolution reaction[J]. Chem. Commun., 2015, 51: 1893 | [5] | Arzac G M, Montes O, Fernández A.Pt-impregnated catalysts on powdery sic and other commercial supports for the combustion of hydrogen under oxidant conditions[J]. Appl. Catal., 2016, 201B: 391 | [6] | Aravind S S J, Ramanujachary K, Mugweru A, et al. Molybdenum phosphide-graphite nanomaterials for efficient electrocatalytic hydrogen production[J]. Appl. Catal., 2015, 490A: 101 | [7] | Deng J, Ren P J, Deng D H, et al.Highly active and durable non-precious-metal catalysts encapsulated in carbon nanotubes for hydrogen evolution reaction[J]. Energy Environ. Sci., 2014, 7: 1919 | [8] | Xiao C H, Li Y B, Lu X Y, et al.Bifunctional porous NiFe/NiCo2O4/Ni foam electrodes with triple hierarchy and double synergies for efficient whole cell water splitting[J]. Adv. Funct. Mater., 2016, 26: 3515 | [9] | Wu C, Li J H.Unique hierarchical Mo2C/C nanosheet hybrids as active electrocatalyst for hydrogen evolution reaction[J]. ACS Appl. Mater. Interfaces, 2017, 9: 41314 | [10] | Gao G P, O'Mullane A P, Du A J. 2D MXenes: A new family of promising catalysts for the hydrogen evolution reaction[J]. ACS Catal., 2017, 7: 494 | [11] | Li W, Xiong D H, Gao X F, et al.Self-supported Co-Ni-P ternary nanowire electrodes for highly efficient and stable electrocatalytic hydrogen evolution in acidic solution[J]. Catal. Today, 2016, 287: 122 | [12] | Zhang C, Huang Y, Yu Y F, et al.Sub-1.1 nm ultrathin porous CoP nanosheets with dominant reactive {200} facets: A high mass activity and efficient electrocatalyst for the hydrogen evolution reaction[J]. Chem. Sci., 2017, 8: 2769 | [13] | Tsai C, Li H, Park S, et al.Electrochemical generation of sulfur vacancies in the basal plane of MoS2 for hydrogen evolution[J]. Nat. Commun., 2017, 8: 15113 | [14] | Ma Q Y, Hu C Y, Liu K L, et al.Identifying the electrocatalytic sites of nickel disulfide in alkaline hydrogen evolution reaction[J]. Nano Energy, 2017, 41: 148 | [15] | Yang Y Q, Zhang K, Lin H L, et al.MoS2-Ni3S2 heteronanorods as efficient and stable bifunctional electrocatalysts for overall water splitting[J]. ACS Catal., 2017, 7: 2357 | [16] | Ho T A, Bae C, Lee S, et al.Edge-on MoS2 thin films by atomic layer deposition for understanding the interplay between the active area and hydrogen evolution reaction[J]. Chem. Mater., 2017, 29: 7604 | [17] | Xiong K, Li L, Zhang L, et al.Ni-doped Mo2C nanowires supported on Ni foam as a binder-free electrode for enhancing the hydrogen evolution performance[J]. J. Mater. Chem., 2015, 3A: 1863 | [18] | Jaramillo T F, J?rgensen K P, Bonde J, et al.Identification of Active edge sites for electrochemical H2 evolution from MoS2 nanocatalysts[J]. Science, 2007, 317: 100 | [19] | Zhang X, Zhang Y, Yu B B, et al.Physical vapor deposition of amorphous MoS2 nanosheet arrays on carbon cloth towards highly reproducible large-area electrocatalysts for the hydrogen evolution reaction[J]. J. Mater. Chem., 2015, 3A: 19277 | [20] | Yu X X, Sun Z J, Yan Z P, et al.Direct growth of porous crystalline NiCo2O4 nanowire arrays on a conductive electrode for high-performance electrocatalytic water oxidation[J]. J. Mater. Chem., 2014, 2A: 20823 | [21] | Gao X H, Zhang H X, Li Q G, et al.Hierarchical NiCo2O4 hollow microcuboids as bifunctional electrocatalysts for overall water-splitting[J]. Angew. Chem., 2016, 55: 6290 | [22] | Wen S Y, Liu Y, Zhu F F, et al.Hierarchical MoS2 nanowires/NiCo2O4 nanosheets supported on Ni foam for high-performance asymmetric supercapacitors[J]. Appl. Surf. Sci., 2018, 428: 616 | [23] | Hu C C, Chen J C, Chang K H.Cathodic deposition of Ni(OH)2 and Co(OH)2 for asymmetric supercapacitors: Importance of the electrochemical reversibility of redox couples[J]. J. Power Sour., 2013, 221: 128 | [24] | Mcarthur M A, Jorge L, Coulombe S, et al.Synthesis and characterization of 3D Ni nanoparticle/carbon nanotube cathodes for hydrogen evolution in alkaline electrolyte[J]. J. Power Sour., 2014, 266: 365 | [25] | Chen J S, Ren J W, Shalom M, et al.Stainless steel mesh-supported NiS nanosheet array as highly efficient catalyst for oxygen evolution reaction[J]. ACS Appl. Mater. Interfaces, 2016, 8: 5509 | [26] | An C H, Wang Y J, Huang Y N, et al.Porous NiCo2O4 nanostructures for high performance supercapacitors via a microemulsion technique[J]. Nano Energy, 2014, 10: 125 | [27] | Liao L, Zhu J, Bian XL, et al.MoS2, formed on mesoporous graphene as a highly active catalyst for hydrogen evolution[J]. Adv. Funct. Mater., 2013, 23: 5326 | [28] | Bose R, Jin Z Y, Shin S, et al.Co-catalytic effects of CoS2 on the activity of the MoS2 catalyst for electrochemical hydrogen evolution[J]. Langmuir, 2017, 33: 5628 | [29] | Lv J L, Meng Y, Liang T X, et al.The effect of reduced graphene oxide on MoS2 for the hydrogen evolution reaction in acidic solution[J]. Chem. Phys. Lett., 2017, 678: 212 | [30] | Chen A S, Cui R J, He Y N, et al.Self-assembly of hollow MoS2 Microflakes by one-pot hydrothermal synthesis for efficient electrocatalytic hydrogen evolution[J]. Appl. Surf. Sci., 2017, 411: 210 | [31] | Bockris J O, Conway B E.The velocity of hydrogen evolution at silver cathodes as a function of hydrogen ion concentration[J]. Trans. Faraday Soc., 1952, 48: 724 | [32] | Yang F, Yao J Y, Liu F L, et al.Ni-Co oxides nanowire arrays grown on ordered TiO2 nanotubes with high performance in supercapacitor[J]. J. Mater. Chem., 2013, 1A: 594 | [33] | Wang J, Zhang L P, Liu X S, et al.Assembly of flexible CoMoO4@NiMoO4 xH2O and Fe2O3 electrodes for solid-state asymmetric supercapacitors[J]. Sci. Rep., 2017, 7: 41088 |
|
|