| 负热膨胀反钙钛矿锰氮化合物的研究综述 |
| 宋晓艳, 孙中华 |
| 北京工业大学材料科学与工程学院新型功能材料教育部重点实验室, 北京 100124 |
|
| REVIEW IN ANTIPEROVSKITE MANGANESE NITRIDES WITH NEGATIVE THERMAL EXPANSION PROPERTIES |
| SONG Xiaoyan, SUN Zhonghua |
| College of Materials Science and Engineering, Key Lab of Advanced Functional Materials, Education Ministry of China, Beijing University of Technology, Beijing 100124 |
引用本文:
宋晓艳 孙中华. 负热膨胀反钙钛矿锰氮化合物的研究综述[J]. 金属学报, 2011, 47(11): 1362-1371.
,
.
REVIEW IN ANTIPEROVSKITE MANGANESE NITRIDES WITH NEGATIVE THERMAL EXPANSION PROPERTIES[J]. Acta Metall Sin, 2011, 47(11): 1362-1371.
| [1] Roy R, Agrawal D K, Mckinstry H A. Annu Rev Mater Sci, 1989; 19: 59[2] Phillips A E, Halder G J, Chapman K W, Goodwin A L, Kepert C J. J Am Chem Soc, 2010; 132: 10[3] Yanase I, Miyagi M, Kobayashi H. J Eur Ceram Soc, 2009; 29: 3129[4] Margadonna S, Prassides K, Fitch A N. J Am Chem Soc, 2004; 126: 15390[5] Salvador J R, Gu F, Hogan T, Kanatzidis M G. Nature, 2003; 425: 702[6] Ramirez I J, Matsumaru K, Ishizaki K. J Ceram Soc Jpn, 2006; 114: 1111[7] Kim I J, Kim H C. J Ceram Process Res, 2004; 5: 308[8] Hummel F A. J Am Ceram Soc, 1951; 51: 235[9] Smith T F, White G K. J Phys, 1975; 8C: 2031[10] White G K. J Phys, 1973; 6D: 2070[11] Mary T A, Evans J S O, Vogt T, Sleight A W. Science, 1996; 272: 90[12] Freiman Y A. Fizika Nizkikh Temp, 1983; 9: 657[13] Wolf F P, Karl V H. Colloid Polym Sci, 1981; 259: 29[14] Choy C L, Chen F C, Young K. J Polym Sci, 1981; 19B: 335[15] Balch D K, Dunand D C. Metall Mater Trans, 2004; 35A: 1159[16] Sonje P U, Subramanian K N, Lee A. J Adv Mater, 2004; 36: 22[17] Sullivan L M, Lukehart C M. Chem Mater, 2005; 17: 2136[18] Chu X X, Huang R J, Yang H H, Wu Z X, Lu J F, Zhou Y, Li L F. Mater Sci Eng, 2011; A528: 3367[19] Yang X B, Xu J, Li H J, Cheng X N, Yan X H. J Am Ceram Soc, 2007; 90: 1953[20] De Buysser K, Lommens P, De Meyer C, Bruneel E, Hoste S, Van Driessche I. Ceram Silik, 2004; 48(4): 139[21] Suzuki T, Omote A. J Am Ceram Soc, 2006; 89: 691[22] Kofteros M, Rodriguez S, Tandon V, Murr L E. Scr Mater, 2001; 45: 369[23] Kumar P S, Kini N S, Umarji A M, Sunandana C S. J Mater Sci, 2006; 41: 3861[24] Aerospace Materials Advisory Research Group. An Advisory Report on the Astronautic and Aeronautic Materials. Beijing: National Defence Industry Press, 1999: 128(航空航天材料咨询研究组. 航空航天材料咨询学报. 北京: 国防工业出版社, 1999: 128)[25] Wang C, Wang T M, Shen R, Liang J K. Physics, 2001; 30: 772(王聪, 王天民, 沈 容, 梁敬魁. 物理, 2001; 30: 772)[26] Sleight A W. Curr Opin Solid State Mater Sci, 1998; 3: 128[27] Sleight A W. Annu Rev Mater Sci, 1998; 28: 29[28] Steele B C H, Heinzel A. Nature, 2001; 414: 345[29] Chen C, Rosenblatt S, Bolotin K I, Kalb W, Kim P, Kymissis I, Stormer H L, Heinz T F, Hone J. Nat Nanotechnol, 2009; 4: 861[30] Allen S, Evans J. Phys Rev, 2003; 68B: 134101[31] Khosrovani K, Sleight A W, Vogt T. J Solid State Chem, 1997; 132: 355[32] Amos T G, Sleight A W. J Solid State Chem, 2001; 160: 230[33] Evans J, Mary T A, Sleight A W. J Solid State Chem, 1998; 137: 148[34] Xing X R, Deng J X, Chen J, Liu G R. Rare Met, 2003; 22: 294[35] Arvanitidis J, Papagelis K, Margadonna S, Prassides K, Fitch A N. Nature, 2003; 425: 599[36] Wen Y C, Wang C, Sun Y, Nie M, Fang L, Tian Y J. Solid State Commun, 2009; 149: 1519[37] Greve B K, Martin K L, Lee P L, Chupas P J, Chapman K W, Wilkinson A P. J Am Chem Soc, 2010; 132: 15496[38] Goodwin A L, Kepert C J. Phys Rev, 2005; 71B: 140301[39] Takenaka K, Takagi H. Appl Phys Lett, 2005; 87: 261902[40] Sun Y, Wang C, Wen Y C, Zhu K G, Zhao J T. Appl Phys Lett, 2007; 91: 231913[41] Bao W Z, Miao F, Chen Z, Zhang H, Jang W Y, Dames C, Lau C N. Nat Nanotechnol, 2009; 4: 562[42] Goodwin A L, Calleja M, Conterio M J, Dove M T, Evans J, Keen D A, Peters L, Tucker M G. Science, 2008; 319: 794[43] Wu Y, Kobayashi A, Halder G J, Peterson V K, Chapman K W, Lock N, Southon P D, Kepert C J. Angew Chem Int Edit, 2008; 47: 8929[44] Das D, Jacobs T, Barbour L J. Nat Mater, 2010; 9: 36[45] Hao Y M, Zhao M, Zhou Y, Hu J F. Scr Mater, 2005; 53: 357[46] Zheng X G, Kubozono H, Yamada H, Kato K, Ishiwata Y, Xu C N. Nat Nanotechnol, 2008; 3: 724[47] Li W H, Wu S Y, Yang C C, Lai S K, Lee K C, Huang H L, Yang H D. Phys Rev Lett, 2002; 89: 135504[48] Forster P M, Yokochi A, Sleight A W. J Solid State Chem, 1998; 140: 157[49] Mary T A, Sleight A W. J Mater Res, 1999; 14: 912[50] Forster P M, Sleight A W. Int J Inorg Mater, 1999; 1: 123[51] Withers R L, Evans J, Hanson J, Sleight A W. J Solid State Chem, 1998; 137: 161[52] Evans J, Hanson J C, Sleight A W. Acta Crystallogr, 1998; 54B: 705[53] Attfield M P, Sleight A W. Chem Mater, 1998; 10: 2013[54] Tao J Z, Sleight A W. J Phys Chem Solids, 2003; 64: 1473[55] Evans J, Hu Z, Jorgensen J D, Argyriou D N, Short S, Sleight A W. Science, 1997; 275: 61[56] Ernst G, Broholm C, Kowach G R, Ramirez A P. Nature, 1998; 396: 147[57] Perottoni C A, Da Jornada J. Science, 1998; 280: 886[58] Sleight A. Nature, 2003; 425: 674[59] Chen J, Xing X R, Sun C, Hu P G, Yu R B, Wang X W, Li L H. J Am Chem Soc, 2008; 130: 1144[60] Takenaka K, Takagi H. Appl Phys Lett, 2009; 94: 131904[61] Huang K, Han R Q. Solid State Physics. Beijing: Higher Education Press, 2004: 137(黄昆, 韩汝琦. 固体物理学. 北京: 高等教育出版社, 2004: 137)[62] Li J, Yokochi A, Amos T G, Sleight A W. Chem Mater, 2002; 14: 2602[63] Tao J Z, Sleight A W. J Solid State Chem, 2003; 173: 442[64] Cai F S. Master Dissertation. Technical Institute of Physics and Chemistry, Chinese Academy of Sciences, Beijing, 2008(蔡方硕.中科院理化技术研究所硕士论文, 北京, 2008)[65] David W, Evans J, Sleight A W. Europhys Lett, 1999; 46: 661[66] Sleight A W. Inorg Chem, 1998; 37: 2854[67] Hao Y M, Zhao M, Zhou Y, Hu J F. Scr Mater, 2005; 53: 357[68] Nakamura Y, Takenaka K, Kishimoto A, Takagi H. J Am Ceram Soc, 2009; 92: 2999[69] Chen J C, Huang G C, Hu C, Weng J P. Scr Mater, 2003; 49: 261[70] Huang R J, Wu Z X, Yang H H, Chen Z, Chu X X, Li L F. Cryogenics, 2010; 50: 750[71] Huang R J, Wu Z X, Chu X X, Yang H H, Chen Z, Li L F. Solid State Sci, 2010; 12: 1977[72] Takenaka K, Asano K, Misawa M, Takagi H. Appl Phys Lett, 2008; 92: 011927[73] Huang R J, Xu W, Xu X D, Li L F, Pan X Q, Evans D. Mater Lett, 2008; 62: 2381[74] Huang R J, Li L F, Cai F S, Xu X D, Qian L H. Appl Phys Lett, 2008; 93: 81902[75] Takenaka K, Takagi H. Mater Trans, 2006; 47: 471[76] Zhang C Y, Zhu J, Zhang M C. Acta Metall Sin, 2009; 45: 97(张从阳, 朱洁, 张茂才. 金属学报, 2009; 45: 97)[77] Sun Z H, Song X Y. Mater Lett, 2009; 63: 2059[78] Song X Y, Sun Z H. China Pat, 200810115717.5, 2008(宋晓艳, 孙中华. 中国专利, 200810115717.5, 2008)[79] Song X Y, Zhang J X, Yue M, Li E D, Zeng H, Lu N D, Zhou M L, Zuo T Y. Adv Mater, 2006; 18: 1210[80] Song X Y, Liu X M, Zhang J X. J Am Ceram Soc, 2006; 89: 494[81] Song X Y, Zhang J X, Li E D, Lu N D, Yin F X. Nanotechnology, 2006; 17: 5584[82] Song X Y, Sun Z H. China Pat, 200910082954.0, 2009(宋晓艳, 孙中华. 中国专利, 200910082954.0, 2009)[83] Sun Z H, Song X Y, Yin F X, Sun L X, Yuan X K, Liu X M. J Phys, 2009; 42D: 122004[84] Sun Z H, Song X Y, Xu L L. Ceram Int, 2011; 37: 1693[85] Song X Y, Liu G Q, He Y Z. Prog Nat Sci, 1998; 8: 92[86] Song X Y, Liu G Q. J Mater Sci, 1999; 34: 2433[87] Song X Y, Gao J P, Zhang J X. Acta Phys Sin, 2005; 54: 1313(宋晓艳, 高金萍, 张久兴. 物理学报, 2005; 54: 1313)[88] Gao J P, Song X Y, Zhang J X. J Mater Sci Technol, 2005; 21: 705[89] Song X Y, Lu N D, Seyring M, Rettenmayr M. Appl Phys Lett, 2009; 94: 023102[90] Sun Y, Wang C, Wen Y C, Chu L H, Pan H, Nie M. J Am Ceram Soc, 2010; 93: 2178[91] Sun Y, Wang C, Wen Y C, Chu L H, Nie M, Liu F. J Am Ceram Soc, 2010; 93: 650[92] Iikubo S, Kodama K, Takenaka K, Takagi H, Shamoto S. Phys Rev, 2008; 77B: 020409[93] Takenaka K, Inagaki T, Takagi H. Appl Phys Lett, 2009; 95: 132508[94] Fruchart D, Bertaut E F. J Phys Soc Jpn, 1978; 44: 781[95] Tahara D, Motome Y, Masatoshi I. J Phys Soc Jpn, 2007; 76: 13708[96] Iikubo S, Kodama K, Takenaka K, Takagi H, Takigawa M, Shamoto S. Phys Rev Lett, 2008; 101: 205901[97] Matsuno J, Takenaka K, Takagi H, Matsumura D, Nishihata Y, Mizuki J. Appl Phys Lett, 2009; 94: 181904[98] Kodama K, Iikubo S, Takenaka K, Takigawa M, Takagi H, Shamoto S. Phys Rev, 2010; 81B: 224419[99] Kittel C. Phys Rev, 1960; 120: 335[100] Sun Y, Wang C, Wen Y C. Mater Sci Forum, 2007; 561– 565: 557[101] Song X Y, Sun Z H, Huang Q Z, Rettenmayr M, Liu X M, Seyring M, Li G N, Rao G H, Yin F X. Adv Mater, 2011; 23: 4690 |
|