| RANDOMNESS AND FUZZINESS OF MESCO DUCTILE FRACTURE FOR METALLIC MATERIALS |
| LU Zhenzhou;YUE Zhufeng;ZHENG Changqing(Northwestern Polytechnical University;Hi'an 710072)(Manuscript received 1996-05-28; in revised form 1996-07-29) |
|
Cite this article:
LU Zhenzhou;YUE Zhufeng;ZHENG Changqing(Northwestern Polytechnical University;Hi'an 710072)(Manuscript received 1996-05-28; in revised form 1996-07-29). RANDOMNESS AND FUZZINESS OF MESCO DUCTILE FRACTURE FOR METALLIC MATERIALS. Acta Metall Sin, 1996, 32(12): 1258-1264.
|
|
|
Abstract Based on the macro-and mesco-experimental results of four steels ,30CrMnSiA,40CrNiMoA,No.45 and No.20,the random and fuzzy properties of fracture are studied.The isolated void model is used as an example,and the fracture occures as the void radius R is greater than the critical Rc. The void radius can be expressed as R=R0exp[C1exp(C2Rσ)εp](R0 is the initial void radius, Rσ the stress triaxiality,εp the plastic strain, C1and C2 are model parameters) .The initial and critical radii of voids are in lognormial distributions and the other parametrs in normal distributions. The calculated fracture characteristics of the four steels in different stress states and strains are more near to the experimental results taking the random fracture model than the deterministic fracture model.The illustrative calculation shows that fuzziness is the nature of fracture state,and with appropriate values the fuzzy model can agree well with the experimental results.
|
|
|
| 1ProvanJW著,航空航天部AFFD系统工程办公室译,概率断裂力学和可靠性.北京:航空工业出版社,1989:2332王光远.工程软设计理论.北京:科学出版社,1990:2393RiceJR,TraceyJ.MechPhysSolids,1969;17:2014郑长卿主编.韧性断裂细观力学的初步研究及其应用.西安:西北工业大学出版社,1988:105周利.见:郑长卿主编,裂纹体与无裂纹体统一断裂理论研究文集,西安:西北工业大学出版社,1991:121 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|