Acta Metall Sin  1996, Vol. 32 Issue (12): 1265-1269    DOI:
Current Issue | Archive | Adv Search |
DIAGRAM OF MICRO-MESO-MACRO MULTILEVEL CONNECTED THEORY OF FRACTURE
XING Xiusan (Beijing Institute of Technology;Beijing 100081)(Manuscript received 1996-01-08;in revised form 1996-06-21)
Cite this article: 

XING Xiusan (Beijing Institute of Technology;Beijing 100081)(Manuscript received 1996-01-08;in revised form 1996-06-21). DIAGRAM OF MICRO-MESO-MACRO MULTILEVEL CONNECTED THEORY OF FRACTURE. Acta Metall Sin, 1996, 32(12): 1265-1269.

Download:  PDF(360KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Starting from nonequilibrium statistical theory of fracture,the block diagram of micro-meso-macro multilevel connected theory of fracture is given.The role of all the different levels and their relationship in the fracture process are described.The transition from micro and meso structures into macro mechanical quantities is exhibited.
Key words:  crystal structure      evolution equation of microcrack      statistical distribution function      macromechanical quantity     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I12/1265

1邢修三.物理学报,1966;22:4872邢修三.物理学报,1980;29:7183邢修三.物理学报,1990:39:16024XingXS.EngFractMech,1986;24:455XingXS.EngFractMech,1987;26:3936邢修三.力学进展,1991,21:1537WeibullW.ProcRoySwedInstEngRes,1939:151:1538KOHTOPOBTA,1941;11:1739 ZhouST,CadssonAE,ThomsonR.PhysRevLett,1994;76:85210HolianBL,RaveloR.PhysRev,1995:B51:11275
[1] Ying LI,Chao SUN,Jun GONG. Performance Research of Magnesium Base Lanthanum Hexaaluminate Prepared by Co-Precipitation[J]. 金属学报, 2019, 55(5): 657-663.
[2] YAO Meiyi, LIN Yuchen, HOU Keke, LIANG Xue, HU Pengfei, ZHANG Jinlong, ZHOU Bangxin. Effect of Sn on Initial Corrosion Behavior of Zirconium Alloy in 280 ℃ LiOH Aqueous Solution[J]. 金属学报, 2019, 55(12): 1551-1560.
[3] Zhen WANG,Bangxin ZHOU,Boyang WANG,Jiao HUANG,Meiyi YAO,Jinlong ZHANG. SECOND PHASE PARTICLES AND THEIR CORROSION BEHAVIOR OF Zr-0.72Sn-0.32Fe-0.15Cr-0.97Nb ALLOY[J]. 金属学报, 2016, 52(1): 78-84.
[4] ZHANG Haixia, LI Zhongkui, ZHOU Lian, XU Bingshe, WANG Yongzhen. EFFECTS OF STRUCTURE AND INTERNAL STRESSES IN OXIDE FILMS ON CORROSION MECHANISM OF NEW ZIRCONIUM ALLOY[J]. 金属学报, 2014, 50(12): 1529-1537.
[5] LI Qiang LIANG Xue PENG Jianchao LIU Renduo YU Kang ZHOU Bangxin. OXIDATION BEHAVIOR OF THE β-Nb PHASE PRECIPITATED IN Zr-2.5Nb ALLOY[J]. 金属学报, 2011, 47(7): 893-898.
[6] PAN Hongge; DU Honglin; CHEN Changpin; HAN Xiufeng; YANG Fuming (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)(Institute of Chinese Atomic Energy; Beijing 102413). STRUCTURAL CHARACTERIZATION OF THE Y_3(Fe, Mo)_(29) INTERMETALLIC COMPOUND[J]. 金属学报, 1998, 34(5): 473-482.
[7] WANG Rongming; LI Chunzhi; PING Dehai; YAN Minggao (Beijing Institute of Aeronautical Materials; Beijing 100095)(Laboratory of Atomic Imaging of Solids; Institute of Metal Research; The Chinese Academy of Sciences;Shenyang 110015)(Beijing Laboratory of Electron Microscopy; The Chinese Academy of Sciences; Beijing 100080). STUDY ON THE PLATELET PHASE IN AN YTTRIUM-CONTAINING LOW EXPANSION SUPERALLOY[J]. 金属学报, 1998, 34(4): 367-372.
[8] XIONG Weihao;HU Zhenhua;CUI Kun (State Key Laboratory of Dies Technology;Huazhong University of Science and Technology; Wuhan 430074). FORMATION MECHANISM OF MICROCRYSTAL INTERFACE LAYER IN Ti(C, N)-BASED CERMET[J]. 金属学报, 1997, 33(5): 473-478.
[9] YANG Xiaoguang; LEI Yongquan; ZHANG Wenkui; ZHU Guangming; WANG Qidong(Zhejiang University; Hangzhou 310027). RELATIONSHIP BETWEEN CRYSTAL CHARACTERISTICS AND ELECTROCHEMICAL PROPERTIES OF Zr BASED HYDROGEN STORAGE ALLOY[J]. 金属学报, 1996, 32(11): 1194-1198.
[10] MAO Jian.fu;HE Liantong;YE Hengqiang(Laboratory of Atomic Imaging of Solids;Ihstitute of Metal Research;Chinese Academy of Sciences;Shenyang 110015) YANG Dezhuang;TANG Zhixiu(Harbin Institute of Technotogy;Harbin 150001)(Manuscript received 1994-07-05;in revised form 1995-02-24). HRTEM STUDY ON CRYSTAL STRUCTURE OF Zr_4Co_4Si_7 COMPOUND[J]. 金属学报, 1995, 31(7): 289-293.
[11] HUANG Jianshun; CHEN Junming (Shanghai Institute of Metallurgy; Academia Sinica). CRYSTAL STRUCTURE OF γ-Li_xFe_2O_3 WITH ELECTROCHEMICAL INSERTION OF Li[J]. 金属学报, 1992, 28(8): 77-83.
No Suggested Reading articles found!