| NEW PROCESS FOR TC11 Ti ALLOY DUAL PROPERTY DISK |
| SU Zuwu; YAO Zekun; GUO Hongzhen; LIU Jianchao(Northwestern Polytechnical University; Xi'an 710072); LIU Jianyu; CUI Jian(Beijing Institute of Aeronautical Materials; Beijing 100095); LIU Guoqing; JIANG Ming; YING Zhiyi(Anda Forging Plant; Anshun; Guizhou 561005) (Manuscript received 1995-08-17; in revised form 1995-11-06) |
|
Cite this article:
SU Zuwu; YAO Zekun; GUO Hongzhen; LIU Jianchao(Northwestern Polytechnical University; Xi'an 710072); LIU Jianyu; CUI Jian(Beijing Institute of Aeronautical Materials; Beijing 100095); LIU Guoqing; JIANG Ming; YING Zhiyi(Anda Forging Plant; Anshun; Guizhou 561005) (Manuscript received 1995-08-17; in revised form 1995-11-06). NEW PROCESS FOR TC11 Ti ALLOY DUAL PROPERTY DISK. Acta Metall Sin, 1996, 32(4): 377-381.
|
|
|
Abstract The dual property TC11 Ti alloy compressor disk of 420 mm in diameter has been manufactured by the techniques of pretreatment and isothermal forging under controllable strain. The disk bore is of the equiaxed structure with high strength, ductility and low-cycle fatigue and the rim with basket-wave microstructure has high resistance to high temperature creep and high fracture toughness. This process is more simple and the production quality is more controllable as comparing with the conventional one. The properties of the bore and rim of the disk is satisfied over the specifications of conventional mechanical properties.Correspondent: YAO Zekun, associate professor, Faculty. No.402, (Northwestern Polytechnical University, Xi'an 710072)
|
|
Received: 18 April 1996
|
| [1]长福主编.航空发动机构造.北京:国防工业出版社,1989:22,97
2LahotiGD,SemiatinSL.OhSI, AltanTIn:HassonDF,NamitionCHeds.,Advanced Processing Casting Forming Machining Welding Methods for Titanium, The Metallurgical Society of AIME,1982:23
3苏祖武,姚泽坤,刘建宇,刘果青.钛合金双性能盘锻造方法.国防专利,91107639.5,1991
4刘建宇,崔健,王贤民,夏诚敬. 见:钛科学与工程,第六届全国钛及钛合金合金学术交流会文集(2),北京:原子能出版社,1987:141
5王金友,葛志明.见:周彦邦编著,航空用钛合金.上海:上海科学技术出版社,1985:210 |