| WETTING AND JOINING OF Sn-BASED ACTIVE SOLDERS ON SIALON CERAMIC IN ROUGH VACUUM |
| ZHUANG Yanxin; XIAN Aiping; WANG Yikang; ZHANG Hiumu; HU Zhuangqi(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-11-03; in revised form 1996-04-15) |
|
Cite this article:
ZHUANG Yanxin; XIAN Aiping; WANG Yikang; ZHANG Hiumu; HU Zhuangqi(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-11-03; in revised form 1996-04-15). WETTING AND JOINING OF Sn-BASED ACTIVE SOLDERS ON SIALON CERAMIC IN ROUGH VACUUM. Acta Metall Sin, 1996, 32(7): 735-741.
|
|
|
Abstract The sessile drop method and four points bending test were used to study the wettability and joining strength of Sn-based solders on Sialon substrates. Under vacuum of 1.33 Pa and holding 20 min at 1173 K, the contact angle of Sn-based is lower than 20 degree,while the joining strength of the soldering joints on rough vacuum may be markedly improved with the addition of zinc or lead, The average joining strength of Sialon/Sialon joints, soldered with Sn-5Cu-STi, Sn-5Cu-5Ti-20Zn, Sn-5Cu-5Ti-10Pb, are 90.8, 154.3 and 169.1 MPa respectively. And the maximums of joining strength are respectively 119.8, 200 and 216.1 MPa for three solders. In rough vacuum, Sn-based active solders may finish the joining of Sialon/Sialon, and the residual stress is reduced. On the other hand, alloy component zinc in Sn-based solders obviously affects precursor film in rough vacuum.Correspondent:ZHUANG Yanxin, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110015
|
|
Received: 18 July 1996
|
| 1DelannayF,ForyenL,DeruvtlereA.JMaterSci,1987,22:12BondleyRJ.CeramicAge,1951;58(1):153TerrillJR,CohranCN,StokesJJ,HaupinWE.WeldJ.1971;50:8334邱惠中.见:中国机械工程学会焊接学会编,第六届全国焊接学术会议选集(第一集),西安,1990:175 KapoorRR,EagarTW.MetallTrans,1989;20B:9196冼爱平.中国科学院金属研究所博士学位论文,1991:977 梁英教.物理化学.北京:冶金工业出版社,1983:808 叶大伦.实用无机物热力学数据手册.北京:冶金工业出版社,1981:289HoweJM.IntMaterRev,1993;38(5):233 |