Acta Metall Sin  1997, Vol. 33 Issue (1): 45-53    DOI:
Current Issue | Archive | Adv Search |
CLASSIFICATION OF THE MARTENSITIC TRANSFORMATIONS
XU Zuyao (T Y.Hsu)(Shanghai Jiaotong University; Shang hai 200030)
Cite this article: 

XU Zuyao (T Y.Hsu)(Shanghai Jiaotong University; Shang hai 200030). CLASSIFICATION OF THE MARTENSITIC TRANSFORMATIONS. Acta Metall Sin, 1997, 33(1): 45-53.

Download:  PDF(868KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Kinetically, martensitic transformation may be classified as athermal and isothermal transformations. According to thermodynamics and interface motion characteristics, martensitic transformation may be divided into thermoelastic, semi-thermoelastic and non-thermoelastic transformations. Criterions for thermoelastic transformation can be drawn as: (1) a small critical driving force and a small hysteresis; (2) reversibility of the motion of the interface between martensite and parent phases. (3) the shape strain is accommodated elastically and the stored energy is available to contribute a part of the driving force for the reverse transformation. From different nucleation processes, the martensitic transformation may be classified as: (1) nucleation nearly through the local soft mode in which the parent strengthening hinders the onset of the transformati0n; and (2) nucleation by stacking fault in which the parent strengthening does not affect the M, markedly and there will not appear a considerable lowering of the Young's modulus at the temperature interval of the internal friction peak exhibition as a result of the martensitic transformation fcc→ hcp. Thequasi-martensitic transformation may be termed for a martensitic transformation with week first order.
Key words:  classification of martensitic transformation      semi-thermoelatic transformation      local soft mode      nucleation by stacking fault      quasi-martensitic transformation     
Received:  18 January 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I1/45

1徐祖耀金属热处理学报,1996;19
2 Christian J W、The Theory of Transformations in Metals and Alloys, Oxford:Pergamon,1965:803
3Lieberman D S.The Mechanism of Phase Iransformations in Crystalline Solids.London:The Inst.Metals,1969 168
4 Cohen M, Olson G B,Clapp P C.Proc Inter Conf on Martensitic Transformations (ICOMAT-79).Cambridge MA:M I T 1979: 1
5 Wayman C M.Mater Sci Forum,1990;56-581
6Olson G B.Mater Sci Forum,1990;56-58:89
7徐祖耀.马氏体相变与马氏体.北京:科学出版社,1980 21
8Delaey L,Chandrasekaran M, Andrade M, Van Humbeeck J. Proc Inter Conf on Solid-Solid PhaseTransformations, New York:AIME,1982; 1429
9Delaey L.In:Hassen P ed,Mater Sci and Tech,Vol.5,Phase Transformations in Materials,1991:339
10Christian J W Mater Sci Eng,1990;A127:215
11Christian J W.In: Wayman C M,Perkins J eds,Proc ICOM A T-92,Monterey Insititute for Advanced Studies, CA U S A 1993: 233
12Brooxs J W,Loretto M J,Smallman R E.Acta Metall 1979; 27: 1829
13Seeger A, Z Metallk,1953;44:247
14Vited V.Phil Mag,1968;773
15徐祖耀,陈明炯.钻及其合金马氏体相变热力学,上海交通大学科研资料,No 80218,1966
16徐祖耀。金属学报,1980;16:430
17Magee C L.Phase Transformations,ASM,1970;115
18 Koistinen D P,Marburger R E Acta Metall 1959; 7: 59
19徐祖耀,吕伟,王永瑞.钢铁,1995;30(4):52
20徐祖耀,李学敏金属学报,1982;19 A83,A505
21Hsu T Y, Li X M. Scr Metall 1982; 17: 1285
22Pati R, Cohen M Acta Metall 1971; 19: 1327
23Entiwisle A R Metall Trans,1971; 2: 2395
24徐祖耀,任怀亮,邓永瑞等北京钢铁学院学报,1960 (1);1
25Hsu T Y, Chen Y, Chen W, Metall Trans,1987 18A: 1389
26Gupta S K Raghavan V.Acta Metall 1975; 23:1239
27徐祖耀金属学报,1991;27 A161
28 Kufdjumov G V,Xandros A N Dokl A H SSSR,1949;66:211
29Kurdiumov G V.J Metals 1959: 449
30 Kaufman L,Cohen M.Prog Metal Phys,Pergamon Press,1958;7:165
31 Hsu T Y J Mater Sci Tech 1994;10:107
32徐祖耀.上海金属,1995;17(6);1
33 Hsu T Y.Mater Scj Forum,1990;56-58:145
34Wu J,Jiang B,Hsu T Y.Acta Metall 1986;36: 1521
35 Tu J,Jiang B Hsu T Y,Zhong J,J Mater Sci,1995;29:1662
36 Reyes-Morel P E,Cherng J S, Chen I-Wei J Am Ceram Soc,1988;71:64837Hayakawa M,Shinmen H Oka M.In:Wayman C M, Perkins J eds,Proc ICOMAT 92 MontereyInstitute for Advanced Studies, CA U S A 1993: 677
38徐祖耀,李箭,曾根朋、金属学报,1986;22 A491
39徐祖耀,陈卫中金属学报,1988;24 A155
40Hsu T Y, Li J;Zen Z Metallography,1986;19: 305
41Hsu T Y,Chen w.Scr Metall,1987;21:1289
42潘牧,徐祖耀金属学报,1984 20:A143
43Hsu T Y,Tan L J Mater Sci,1983;18:3213
44徐祖耀,颜林发金属学报,1986;24 A143
45颜林发,徐祖耀.金属学报,1986;22 A385
46Hsu T Y,Yan L,Metallography,1984;17:397
47陈树川,徐祖耀,杨凡,张骥华。金属学报, 1991; 27; A249
48Chen W, Hsu T Y, Chen S, Zhang J Acta Metall Mater,1990; 38:2337
49Clapp P C.Phys Stat Sol(b), 1973; 57: 56
50徐祖耀。相变原理,北京:科学出版社,1988;1:501
51Jiang B H, Qi X, Zhou W, Hsu T Y. Scr Mater, 1996; 34 771
52Hsu T Y, Chen S Chung C Y to be published
53 Yoshida I,Otsuka H.J Alloys compounds,1994;211-212:208
54Perez-Saez R B No M L,Juan J San J Alloys Compounds,1994 211-212: 2126
No related articles found!
No Suggested Reading articles found!