| CLASSIFICATION OF THE MARTENSITIC TRANSFORMATIONS |
| XU Zuyao (T Y.Hsu)(Shanghai Jiaotong University; Shang hai 200030) |
|
Cite this article:
XU Zuyao (T Y.Hsu)(Shanghai Jiaotong University; Shang hai 200030). CLASSIFICATION OF THE MARTENSITIC TRANSFORMATIONS. Acta Metall Sin, 1997, 33(1): 45-53.
|
|
|
Abstract Kinetically, martensitic transformation may be classified as athermal and isothermal transformations. According to thermodynamics and interface motion characteristics, martensitic transformation may be divided into thermoelastic, semi-thermoelastic and non-thermoelastic transformations. Criterions for thermoelastic transformation can be drawn as: (1) a small critical driving force and a small hysteresis; (2) reversibility of the motion of the interface between martensite and parent phases. (3) the shape strain is accommodated elastically and the stored energy is available to contribute a part of the driving force for the reverse transformation. From different nucleation processes, the martensitic transformation may be classified as: (1) nucleation nearly through the local soft mode in which the parent strengthening hinders the onset of the transformati0n; and (2) nucleation by stacking fault in which the parent strengthening does not affect the M, markedly and there will not appear a considerable lowering of the Young's modulus at the temperature interval of the internal friction peak exhibition as a result of the martensitic transformation fcc→ hcp. Thequasi-martensitic transformation may be termed for a martensitic transformation with week first order.
|
|
Received: 18 January 1997
|
1徐祖耀金属热处理学报,1996;19 2 Christian J W、The Theory of Transformations in Metals and Alloys, Oxford:Pergamon,1965:803 3Lieberman D S.The Mechanism of Phase Iransformations in Crystalline Solids.London:The Inst.Metals,1969 168 4 Cohen M, Olson G B,Clapp P C.Proc Inter Conf on Martensitic Transformations (ICOMAT-79).Cambridge MA:M I T 1979: 1 5 Wayman C M.Mater Sci Forum,1990;56-581 6Olson G B.Mater Sci Forum,1990;56-58:89 7徐祖耀.马氏体相变与马氏体.北京:科学出版社,1980 21 8Delaey L,Chandrasekaran M, Andrade M, Van Humbeeck J. Proc Inter Conf on Solid-Solid PhaseTransformations, New York:AIME,1982; 1429 9Delaey L.In:Hassen P ed,Mater Sci and Tech,Vol.5,Phase Transformations in Materials,1991:339 10Christian J W Mater Sci Eng,1990;A127:215 11Christian J W.In: Wayman C M,Perkins J eds,Proc ICOM A T-92,Monterey Insititute for Advanced Studies, CA U S A 1993: 233 12Brooxs J W,Loretto M J,Smallman R E.Acta Metall 1979; 27: 1829 13Seeger A, Z Metallk,1953;44:247 14Vited V.Phil Mag,1968;773 15徐祖耀,陈明炯.钻及其合金马氏体相变热力学,上海交通大学科研资料,No 80218,1966 16徐祖耀。金属学报,1980;16:430 17Magee C L.Phase Transformations,ASM,1970;115 18 Koistinen D P,Marburger R E Acta Metall 1959; 7: 59 19徐祖耀,吕伟,王永瑞.钢铁,1995;30(4):52 20徐祖耀,李学敏金属学报,1982;19 A83,A505 21Hsu T Y, Li X M. Scr Metall 1982; 17: 1285 22Pati R, Cohen M Acta Metall 1971; 19: 1327 23Entiwisle A R Metall Trans,1971; 2: 2395 24徐祖耀,任怀亮,邓永瑞等北京钢铁学院学报,1960 (1);1 25Hsu T Y, Chen Y, Chen W, Metall Trans,1987 18A: 1389 26Gupta S K Raghavan V.Acta Metall 1975; 23:1239 27徐祖耀金属学报,1991;27 A161 28 Kufdjumov G V,Xandros A N Dokl A H SSSR,1949;66:211 29Kurdiumov G V.J Metals 1959: 449 30 Kaufman L,Cohen M.Prog Metal Phys,Pergamon Press,1958;7:165 31 Hsu T Y J Mater Sci Tech 1994;10:107 32徐祖耀.上海金属,1995;17(6);1 33 Hsu T Y.Mater Scj Forum,1990;56-58:145 34Wu J,Jiang B,Hsu T Y.Acta Metall 1986;36: 1521 35 Tu J,Jiang B Hsu T Y,Zhong J,J Mater Sci,1995;29:1662 36 Reyes-Morel P E,Cherng J S, Chen I-Wei J Am Ceram Soc,1988;71:64837Hayakawa M,Shinmen H Oka M.In:Wayman C M, Perkins J eds,Proc ICOMAT 92 MontereyInstitute for Advanced Studies, CA U S A 1993: 677 38徐祖耀,李箭,曾根朋、金属学报,1986;22 A491 39徐祖耀,陈卫中金属学报,1988;24 A155 40Hsu T Y, Li J;Zen Z Metallography,1986;19: 305 41Hsu T Y,Chen w.Scr Metall,1987;21:1289 42潘牧,徐祖耀金属学报,1984 20:A143 43Hsu T Y,Tan L J Mater Sci,1983;18:3213 44徐祖耀,颜林发金属学报,1986;24 A143 45颜林发,徐祖耀.金属学报,1986;22 A385 46Hsu T Y,Yan L,Metallography,1984;17:397 47陈树川,徐祖耀,杨凡,张骥华。金属学报, 1991; 27; A249 48Chen W, Hsu T Y, Chen S, Zhang J Acta Metall Mater,1990; 38:2337 49Clapp P C.Phys Stat Sol(b), 1973; 57: 56 50徐祖耀。相变原理,北京:科学出版社,1988;1:501 51Jiang B H, Qi X, Zhou W, Hsu T Y. Scr Mater, 1996; 34 771 52Hsu T Y, Chen S Chung C Y to be published 53 Yoshida I,Otsuka H.J Alloys compounds,1994;211-212:208 54Perez-Saez R B No M L,Juan J San J Alloys Compounds,1994 211-212: 2126 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|