| THE APB ENERGIES OF Ni_(74.5)Pd_2Al_(23.5) ALLOY WITH L1_2 STRUCTURE |
| SUN Jian(The Public Laboratory of State Education Commission.for High Temperature Materials and High Temperature Tests;Shanghai Jiaotong University; Shanghai 200030); C. S. Lee; J. K. L. Lai(City University of Hong Kong; Hong Kong) |
|
Cite this article:
SUN Jian(The Public Laboratory of State Education Commission.for High Temperature Materials and High Temperature Tests;Shanghai Jiaotong University; Shanghai 200030); C. S. Lee; J. K. L. Lai(City University of Hong Kong; Hong Kong). THE APB ENERGIES OF Ni_(74.5)Pd_2Al_(23.5) ALLOY WITH L1_2 STRUCTURE. Acta Metall Sin, 1997, 33(11): 1130-1134.
|
|
|
Abstract Using the TEM weak beam technigue,the APB energies on the (111) and (100) planes of Ni74.5Pd2A123.5 alloy with L12 structure were determined to be(144±20) mJ / m2 and (102±11) mJ/m2 respectively.The relation of ordering energies on the ductility of the alloy was also discussed in this paper.
|
|
Received: 18 November 1997
|
1ChibaA,HanadaS,WatanbeS.MaterTransJIM,1991;39:824 2ChibaA,HanadaS,WatanbeS.BullJpnInstMet,1991;30:12 3KearBH,WilsdorfHG.TransMetallSocAIME,1962;224:382 4HirthJP,LotheJ.TheoryofDislocations.2nded,NewYork:John-Wiley&Sons,1982:423 5YooMN.ActaMetall,1987;35:1559 6DimidukDM,ThompsonAW,WilliamsJC.PhilosMag,1993;A67:675_ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|