Please wait a minute...
Acta Metall Sin  1997, Vol. 33 Issue (11): 1130-1134    DOI:
Current Issue | Archive | Adv Search |
THE APB ENERGIES OF Ni_(74.5)Pd_2Al_(23.5) ALLOY WITH L1_2 STRUCTURE
SUN Jian(The Public Laboratory of State Education Commission.for High Temperature Materials and High Temperature Tests;Shanghai Jiaotong University; Shanghai 200030); C. S. Lee; J. K. L. Lai(City University of Hong Kong; Hong Kong)
Cite this article: 

SUN Jian(The Public Laboratory of State Education Commission.for High Temperature Materials and High Temperature Tests;Shanghai Jiaotong University; Shanghai 200030); C. S. Lee; J. K. L. Lai(City University of Hong Kong; Hong Kong). THE APB ENERGIES OF Ni_(74.5)Pd_2Al_(23.5) ALLOY WITH L1_2 STRUCTURE. Acta Metall Sin, 1997, 33(11): 1130-1134.

Download:  PDF(1554KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Using the TEM weak beam technigue,the APB energies on the (111) and (100) planes of Ni74.5Pd2A123.5 alloy with L12 structure were determined to be(144±20) mJ / m2 and (102±11) mJ/m2 respectively.The relation of ordering energies on the ductility of the alloy was also discussed in this paper.
Key words:  APB energy      Ni_3Al intermetallic compound      TEM weak beam technique     
Received:  18 November 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I11/1130

1ChibaA,HanadaS,WatanbeS.MaterTransJIM,1991;39:824
2ChibaA,HanadaS,WatanbeS.BullJpnInstMet,1991;30:12
3KearBH,WilsdorfHG.TransMetallSocAIME,1962;224:382
4HirthJP,LotheJ.TheoryofDislocations.2nded,NewYork:John-Wiley&Sons,1982:423
5YooMN.ActaMetall,1987;35:1559
6DimidukDM,ThompsonAW,WilliamsJC.PhilosMag,1993;A67:675_
[1] ZENG Chaoliu; ZHANG Jianqing;WU Weitao; NIU Yan(Corrosion Science Lab Oratory; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang). ELECTROCHEMICAL IMPEDANCE OF HOT CORROSION OF SPUTTERED CoCrAlY COATING ON Ni_3Al And Ni_3Al-Fe INTERMETALLICS[J]. 金属学报, 1994, 30(18): 247-253.
No Suggested Reading articles found!