Please wait a minute...
Acta Metall Sin  1997, Vol. 33 Issue (9): 912-916    DOI:
Current Issue | Archive | Adv Search |
INTERNAL FRICTION SPECTRUM OF THE INTERSTITIAL FREE COLD-ROLLED STEEL FOR AUTOMOBILE
ZENG Guiyi;CHE Yunyi;JIN Hongzheng;JI Jingwen(Northeastern University;Shenyang 110006); HUANG Zhenru;LIU Jianmin;HUA Qiaozhu;ZHOU Xing(Research Institute of Iron and Steel; Baoshan Iron and Steel Company;Shanghai 201900)
Cite this article: 

ZENG Guiyi;CHE Yunyi;JIN Hongzheng;JI Jingwen(Northeastern University;Shenyang 110006); HUANG Zhenru;LIU Jianmin;HUA Qiaozhu;ZHOU Xing(Research Institute of Iron and Steel; Baoshan Iron and Steel Company;Shanghai 201900). INTERNAL FRICTION SPECTRUM OF THE INTERSTITIAL FREE COLD-ROLLED STEEL FOR AUTOMOBILE. Acta Metall Sin, 1997, 33(9): 912-916.

Download:  PDF(471KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The spectrum of internal friction in a interstital free cold-rolled steel produced by Baoshan Iron and Steel Companay (BIF) for automobile has been studied. The results showed that a Snoek-Ke-Koster peak appears for in situ annealing steel at 900℃ and there are different influences of magnetic field on the internal friction in the specimens annealed at 700℃ and 720℃.
Key words:  nternal friction      steel for automobile      deep drawing sheet     
Received:  18 September 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I9/912

1戢景文,李尚诣物理,1995;124:599
2Ke T S Trans AIME 1948;176:44
3Wang Y N,Zhu J S J de phys,1981;40:C5-457
4戢景文,樊文杰,吴玉琴,王辉东工学院学报,1991;12:1784
5Petarra D P,Bechers D N Acta Metall 1967;15:791
6戢景文,魏全金,张国福,赖祖涵,陈挺国金属学报,1992;28:A207
7Ino H Segeno T Acta Metall,1967;15:1197
8戢景文,赵增祺,贺礼瑞,耿殿奇物理学报,1985;34:162
9Niblett D H,Wilks J Adv Phys,1960;9(1):1
10戢景文,孙玉杰,刘艳美金属学报,1994;30:A210
11Fischbach D B Acta Metall,1962;10:319
[1] LI Weijuan, ZHANG Hengyi, FU Hao, ZHANG Jianping, QI Xiangyu. INTERNAL FRICTION STUDY OF MECHANISM OF BAKE-HARDENING ON LOW CARBON STEEL[J]. 金属学报, 2015, 51(4): 385-392.
[2] WANG Hua SHI Wen HE Yanlin FU Renyu LI Lin. STUDY OF Mn AND P SOLUTE DISTRIBUTIONS AND THEIR EFFECT ON THE TENSILE BEHAVIOR IN ULTRA LOW CARBON BAKE HARDENING STEELS[J]. 金属学报, 2011, 47(3): 263-268.
[3] WU Jie CUI Hongzhi CHI Jing YAO Shuyu HAN Fusheng. INTERNAL FRICTION PEAK IN B2 Fe--Al ALLOYS DURING ORDERING PROCESS[J]. 金属学报, 2009, 45(4): 396-399.
[4] Jian ZHANG. EFFECTS OF GRAIN-BOUNDARY PHASES ON HYDROGEN EMBRITTLEMENT OF FE-NI-CR AUSTENITIC ALLOY BY INTERNAL FRICTION[J]. 金属学报, 2008, 44(9): 1095-1098 .
[5] SUN Wei. The internal friction peak correlated to the relaxation of Al antisite atoms in Fe-Al alloys[J]. 金属学报, 2007, 43(3): 311-314 .
[6] WANG Hongbin; WANG Xiaoyu; ZHANG Jihua; XU Zuyao T. Y. Hsu. Internal Friction of Nano--Grained Fe--25\%Ni Alloy Bulk[J]. 金属学报, 2004, 40(5): 523-526 .
[7] CHE Yunyi; LIU Fendi; ZENG Guiyi; XU Yuchang; JI Jingwen (College of Sciences; Northeastern Univerisity; Shenyang 110006)HUA Qiaozhu; LIU Jianmin; HUANG Zhenru(Institute of Iron & Steel; Baoshan Iron & Steel Company; Shanghai 201900)Correspondent: JI Jingwen; professor; Tel: (024)25915148; Fax: (024)23891072;E-mail: cos ramm. cneu. edu. cn.. Snoek-K■-kster DAMPING IN 340 MPa BAKE HARDENING STEELS[J]. 金属学报, 1998, 34(8): 831-835.
[8] WANG Weiguo; ZHOU Bangxin; ZHENG Zhongmin(Laboratory for Nuclear Fuel and Materials; Nuclear Power Institute of China; Chengdu 610041)Correspondent: WANG Weiguo; Tel: (028)5582199-88531. DAMPING CAPACITY OF Fe-Cr-Al-Si ALLOYS[J]. 金属学报, 1998, 34(10): 1039-1042.
[9] YUAN Lixi; FANG Qianfeng(Laboratory of Internal Fricion and Defects in Solids;Institute of Solid State Physics; The Chinese Academy of Sciences; Hefei 230031) Correspondents: FANG Qianfeng;professor;E-mail:qffang@issp.hfcas.ac.cn. NONLINEAR FITTING OF THE INTERNAL FRICTION DATA AND ITS APPLICATION ON THE BAMBOO GRAIN BOUNDARY RELAXATION IN PURE Al[J]. 金属学报, 1998, 34(10): 1016-1020.
[10] GE Tingsui (T S. KE); (Laboratory of Internal Friction and Defects in Solinds; Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031). EXPERIMENTAL AND THEORETICAL STUDY ON NON-LINEAR ANELASTIC INTERNAL FRICTION[J]. 金属学报, 1997, 33(1): 9-21.
[11] LIU Junmin; ZHANG Jinxiu (Zhongshan University; Guangzhou 510275)(Manuscript received 1995-08-09; in revised form 1996-04-11). BHAVIOUR OF COMPLEX ELASTIC MODULUS AND INTERNAL FRICTION DURING EUTECTOID DECOMPOSITION[J]. 金属学报, 1996, 32(8): 785-790.
[12] LIU Junmin(Department of Physics; Zhongshan University; Guangzhou 510275);SHUI Jiapeng(Institute of Solid State Physics; Chinese Academy of Sciences; Hefei230031)(Manuscript received 1994-04-15). STRUCTURE RELAXATION OF AMORPHOUS ALLOYS[J]. 金属学报, 1995, 31(19): 318-323.
[13] JI Jingwen;SUN Yujie;LIU Yanmei(Northeastern University; Shenyang)(Manuscript received 7 September; 1993; in revised form 10 December;1993). HIGH TEMPERATURE INTERNAL FRICTION FOR Fe-Nb-C ALLOYS[J]. 金属学报, 1994, 30(5): 210-216.
[14] GUAN Xingsheng;GE Tingsui (T. S. Ke) Laboratory of Internal Friction and Defects in Solids; Institute of Solid State Physics; Academia Sinica; HefeiInstitute of Solid State Physics; Academia Sinica; Hefei 230031. INTERNAL FRICTION PEAK ASSOCIATED WITH GRAIN BOUNDARY IN Al BICRYSTALS[J]. 金属学报, 1993, 29(8): 1-4.
[15] SHUI Jiapeng; CHENG Lifang; LIU Junmin; CHU Zhaoqin (Institute of Solid State Physics; Academia Sinica; Hefei). STABILITY OF NANOCRYSTALLINE Ni-P RIBBON[J]. 金属学报, 1992, 28(9): 73-76.
No Suggested Reading articles found!