ANALYSIS OF THE ELASTO-PLASTIC PROPERTIES AND COMPUTATIONAL MODELS FOR TWO-PHASE COMPOSITES
ZHOU Zhe(Northern Jiaotong University; Beijing 100044); KUANG Zhenbang (Shanghai Jiaotong University); Shanghai 200030)
Cite this article: 

ZHOU Zhe(Northern Jiaotong University; Beijing 100044); KUANG Zhenbang (Shanghai Jiaotong University); Shanghai 200030). ANALYSIS OF THE ELASTO-PLASTIC PROPERTIES AND COMPUTATIONAL MODELS FOR TWO-PHASE COMPOSITES. Acta Metall Sin, 1997, 33(9): 903-911.

Download:  PDF(734KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A three region model was proposed to study elasto-plastic mechanical behavior of two-phase composites by finite deformation FEM. The influences of two region model,three region model and periodic distribution particle model on the calculated results were compared. The effects of shape, distribution and volume fraction of inclusions on the elasto-plastic mechanical behavior were analyzed. The results obtained in this paper are important for understanding macro-behavior of two phase composites.
Key words:  two-phase composite      elasto-plastic mechanical behavior      three regionmodel finite element method     
Received:  18 September 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I9/903

1Eshelby J D.Proc roy soc,1957;A241:376
2Hill R.J.Mech Phys Solids,1965;13:213
3Mori T,Tanaka K.Acta metall ,1973;21:571
4Tandon G P,Weng G J Appl Mech 1988;55:126
5Shen Y L ,Finot M,Needleman A,Suresh S.Acta Metall Mater,199443:1701
6Dutta I,Sims J D,Seigenthaler D M.Acta Metall Mater,1993;41:885
7Smith J D.J Res National Bureau Standard 1974 78A: 355
8匡震邦.非线性连续介质力学基础西安:西安交通大学出版社,1989:140
No related articles found!
No Suggested Reading articles found!