| CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS |
| Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083) |
|
Cite this article:
Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083). CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS. Acta Metall Sin, 1998, 34(1): 75-85.
|
|
|
Abstract After combining investigation of thermodynamic properties of binary metallic melts with their phase diagrams, it has been found that when the calculating models of mass action concentrations of metallic melts are formulated according to their main phase diagrams (i.e.phase diagrams involving compound formation, involving peritectic, involving saturated phase,involving solid solution and involving eutectic), the calculated thermodynamic properties (mass action concentrations) will rigorously obey the mass action law, except for the continuous solid solution obeying Raoult's law.
|
|
Received: 18 January 1998
|
1 Baker H.Okamoto H,Henry S D,Davidson G M,Fleming M A;Kacprzak L,Lampman H F,Scott W W Jr,Uhr R C.ASM Handbook Vol.3,Materials Park,Ohio:The Materials Information Society,1992:225 2 Massalski T B, Murry T L,Bennet L N;Baker H.Binary Alloy Phase Diagrams, Metals Park,Ohio:American Society for Metals;1986:1 3 张鉴.炉外精炼的理论与实践 北京:冶金工业出版社,1993:103(Zhang Jian.Theory and Practice of Refining Outside Furnace.Beijing:Metallurgical Industry Press;1993:103) 4 张鉴.特殊钢,1994;16(6):43(Zhang Jian.Special Steel,1994; 16(6): 43) 5 张鉴、钢铁研究学报,19912 3(2):7(Zhang Jian.J Steel Iron Res;1991; 3(2): 7 6 Chipman J,Fulton J C,Gokcen N A,Gaskey G R.Acta Metall,1954; 2:439 7 张鉴中国有色金属学报,19972 7:(Zhang Jian.Chin J Nonfer Met,1997;7:) 8 Hultgren R,Desai P D,Hawkins D T,Gleiser M,Kelley K K.Selected Values of the ThermodynamicProperties of Binary Alloys,Metal Park,Ohio:American Society for Metals,1973:299 9 成国光,张鉴.庆祝朱觉教授八十寿辰论文集.北京:冶金工业出版社,1994:147(Cheng Guoguang,Zhang Jian.Proceedings of Eightyth Birthday of Professor Zhu Jue.Beijing:Metallurgical Industry Press; 1994: 147) 10 成国光,张鉴.特殊钢,1993;14(3):9(Cheng Guoguang,Zhang Jian.Special Special Steel,1993;14(3): 9) 11 Zhang Jian.J Uni Sci Technol Beijing,1994, 1(1-2):22 12 张鉴 1994年全国冶金物理化学学术会议论文集,中国广州,1994:122(Zhang Jian.Proceedings of Chinese Conference on Chemistry and Physics of MetallurgicalProcess,1994,Guangzhou,China 1994:122) 13 Nash P,Singleton M F Bulloy Phase Diagrams,1989;10:258 14 Lundin C E,Yamamoto A S,Nachman J F.Acta Metall,1965; 13: 149 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|