CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS
Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083)
Cite this article: 

Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083). CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS. Acta Metall Sin, 1998, 34(1): 75-85.

Download:  PDF(888KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  After combining investigation of thermodynamic properties of binary metallic melts with their phase diagrams, it has been found that when the calculating models of mass action concentrations of metallic melts are formulated according to their main phase diagrams (i.e.phase diagrams involving compound formation, involving peritectic, involving saturated phase,involving solid solution and involving eutectic), the calculated thermodynamic properties (mass action concentrations) will rigorously obey the mass action law, except for the continuous solid solution obeying Raoult's law.
Key words:  metallic melt      phase diagram      coexistence theory      mass action concentration     
Received:  18 January 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I1/75

1 Baker H.Okamoto H,Henry S D,Davidson G M,Fleming M A;Kacprzak L,Lampman H F,Scott W W Jr,Uhr R C.ASM Handbook Vol.3,Materials Park,Ohio:The Materials Information Society,1992:225
2 Massalski T B, Murry T L,Bennet L N;Baker H.Binary Alloy Phase Diagrams, Metals Park,Ohio:American Society for Metals;1986:1
3 张鉴.炉外精炼的理论与实践 北京:冶金工业出版社,1993:103(Zhang Jian.Theory and Practice of Refining Outside Furnace.Beijing:Metallurgical Industry Press;1993:103)
4 张鉴.特殊钢,1994;16(6):43(Zhang Jian.Special Steel,1994; 16(6): 43)
5 张鉴、钢铁研究学报,19912 3(2):7(Zhang Jian.J Steel Iron Res;1991; 3(2): 7
6 Chipman J,Fulton J C,Gokcen N A,Gaskey G R.Acta Metall,1954; 2:439
7 张鉴中国有色金属学报,19972 7:(Zhang Jian.Chin J Nonfer Met,1997;7:)
8 Hultgren R,Desai P D,Hawkins D T,Gleiser M,Kelley K K.Selected Values of the ThermodynamicProperties of Binary Alloys,Metal Park,Ohio:American Society for Metals,1973:299
9 成国光,张鉴.庆祝朱觉教授八十寿辰论文集.北京:冶金工业出版社,1994:147(Cheng Guoguang,Zhang Jian.Proceedings of Eightyth Birthday of Professor Zhu Jue.Beijing:Metallurgical Industry Press; 1994: 147)
10 成国光,张鉴.特殊钢,1993;14(3):9(Cheng Guoguang,Zhang Jian.Special Special Steel,1993;14(3): 9)
11 Zhang Jian.J Uni Sci Technol Beijing,1994, 1(1-2):22
12 张鉴 1994年全国冶金物理化学学术会议论文集,中国广州,1994:122(Zhang Jian.Proceedings of Chinese Conference on Chemistry and Physics of MetallurgicalProcess,1994,Guangzhou,China 1994:122)
13 Nash P,Singleton M F Bulloy Phase Diagrams,1989;10:258
14 Lundin C E,Yamamoto A S,Nachman J F.Acta Metall,1965; 13: 149
[1] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[2] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[3] ZHANG Huawei; LI Yanxiang; LIU Yuan. Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. 金属学报, 2005, 41(1): 55-.
[4] ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(7): 742-752.
[5] ZHOU Hong; WANG Jinguo; JIA Shusheng (Jilin University of Technology; Chanerhun 130025) OGIKeisaku(Kyushu Universily; Japan) (Manuscript received 1996-03-22; in revised form 1997-04- 13). SOLIDIFIED MICROSTRUCTURES AND PHASES OF HIGH SPEED STEELS CONTA1NING DIFFERENT V AND C CONTENT[J]. 金属学报, 1997, 33(8): 838-843.
[6] ZHANG Jian (University of Science and Technology Beijing; Beijing 100083). CALCULATING MODELS OF MASS ACTION CONCENTRATIONS FOR SEVERAL MOLTEN BINARY SALTS[J]. 金属学报, 1997, 33(5): 515-523.
[7] FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10). KPO_3-M0O_3 PHASE DIAGRAM[J]. 金属学报, 1997, 33(4): 395-397.
[8] ZHOU Guozhi(Kuo-Chih Chou) (University of Science and Technology Beijing;Beiing 100083). NEW GENERATION SOLUTION GEOMETRICAL MODEL AND ITS FURTHER DEVELOPMENT[J]. 金属学报, 1997, 33(2): 126-132.
[9] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
[10] YUAN Wenxia; MA Shulan; QIAO Hin; ZHUANG Weidong; XING Xianran;QIAO Zhiyu (University of Science and Technology Beijing; Beijing 100083)(General Institute for Non-Ferrous Metals; Beijing 100088)(Manuscript received 1995-04-28; in revised form 1995-11-05). A STUDY ON THE YCl_3-AECl_2(AE=Mg, Ca, Sr, Ba)BINARY PHASE DIAGRAMS[J]. 金属学报, 1996, 32(2): 139-143.
[11] HAO Shiming; ZENG Ninghua (Northeastern University; Shenyang 110006)(Manuscript received 1994-11-16). ISOTHERMAL SECTION OF PHASE DIAGRAM IN Ti-Al-Cr TERNARY SYSTEM AT 1000℃[J]. 金属学报, 1995, 31(16): 152-158.
[12] YAN Licheng;FANG Jianhui;XU Jingyan;YANG Jinxiu(Shanghai University of Science and Technology). PHASE DIAGRAM OF KF-LiCl-CaCl_2 SYSTEM[J]. 金属学报, 1994, 30(19): 301-303.
[13] WAN Jinglong(Anhui Institute of Technology; Hefei); BI Qinghua(Shanghai University of Science and Technology). Gd-CoAl VERTICAL SECTION OF Gd-Co-Al PHASE DIAGRAM[J]. 金属学报, 1994, 30(17): 204-207.
[14] XU Qian;YU Yaxin;QIU Zhuxian(Northeastern University;Shenyang)(Manuscript received 25 June;1993). THERMODYNAMIC PROPERTIES AND PHASE DIAGRAMS OF Li-CaF_2,NaF-CaF_2 AND KF-CaF_2[J]. 金属学报, 1994, 30(16): 150-155.
[15] SHEN Jianyun(General Research Institute for Non-Ferrous Metals;Beijing);CHATILLON C(Laboratoire de Thermodynamique et Physico-chimie Metallurgiques;Fracne)(Manuscript received 16 June;1993). THERMODYNAMICS OF Ga-In-As SYSTEM UNDER LATTICE DEFORMATION[J]. 金属学报, 1994, 30(16): 145-149.
No Suggested Reading articles found!