Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (2): 141-145    DOI:
Current Issue | Archive | Adv Search |
ENVIRONMEMTAL EMBRITTLEMENT AND HYDROGEN DIFFUSION IN Co_3Ti ALLOYS
WAN Xiaojing;CHENG Xiaoying;CHEN Yexin (Institute of Meterials Science; Shanghai University; Shanghai 200072)
Cite this article: 

WAN Xiaojing;CHENG Xiaoying;CHEN Yexin (Institute of Meterials Science; Shanghai University; Shanghai 200072). ENVIRONMEMTAL EMBRITTLEMENT AND HYDROGEN DIFFUSION IN Co_3Ti ALLOYS. Acta Metall Sin, 1998, 34(2): 141-145.

Download:  PDF(1333KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of boron doping on the sensitivity to environmental embrittlement of Co3Ti alloys was investigated. The results show that the boron doping in Co3Ti does not have the effect on suppressing environmental embrittlement. The hydrogen diffusion coefficients in Co3Ti alloys with and without boron measured by a new experimental method have almost the same value, which indicates that boron in Co3Ti alloys does not reduce the hydrogen diffusivity along the grain boundaries. The susceptibility of boron-doped Co3Ti alloys to moisture-induced environmental embrittlement is attributed to no boron atoms segregating to the grain boundaries.
Key words:  Co_3Ti      environmental embrittlement      hydrogen diffusivity     
Received:  18 February 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I2/141

1George E P,Liu C T,Pope D P.Scripta Metall,1993;28:875
2 Wan X J, Zhu J H, Jing K L. Scr Metall 1992; 26: 473
3Takasugi,T ,Izumi O.Acta Metall,1986;3:607
4Tasasugi T, Izumi O, Yashida M.J Mater Sci,1991; 26: 1173
5 Wan X J, Zhu J H, Jing K L, Chen W J, Wu Y.J Mater Sci Technol 1994; 10: 39
6万晓景,朱家红,黄胜标.金属学报,1995;31:B183 (Wan X J, Zhu J H, Huang S B、 Acta Metall Sin, 1995; 31: B183)
7Wan X J, Zhu J H, Huang S B. Acta Metall Sin(Eng Lett), 1995; 8: 299
8Liu C T, White C L, Horton J A. Acta Mete 1985; 33: 213
9Wan X J, Zhu J H, Jing K L. Scr Metall Mater 1994; 31: 677
10Takasugi T, Hono K, Suzch S, Hanada S, Sukurai T. Scr Metall , 1993; 29: 1587
11Takasugi T, Takazawa M, Izumi O.J Mater Sci, 1990; 25: 4239
12Zhu J H, Wan X J, Wu Y. Scr Metalll Mater 1993; 29: 429
13George E P,Liu C T.Mat Res Soc Symp Proc,1995; 364:1131`
[1] ZHU Jiahong;WAN Xiaojing(Shanghai University of Technology)(Manuscript received 1 April;1993;in revised form 8 July;1993). ENVIRONMENTAL EMBRITTLEMENT IN Fe_3Al BASED ALLOYS[J]. 金属学报, 1994, 30(3): 139-144.
No Suggested Reading articles found!