| ENVIRONMEMTAL EMBRITTLEMENT AND HYDROGEN DIFFUSION IN Co_3Ti ALLOYS |
| WAN Xiaojing;CHENG Xiaoying;CHEN Yexin (Institute of Meterials Science; Shanghai University; Shanghai 200072) |
|
Cite this article:
WAN Xiaojing;CHENG Xiaoying;CHEN Yexin (Institute of Meterials Science; Shanghai University; Shanghai 200072). ENVIRONMEMTAL EMBRITTLEMENT AND HYDROGEN DIFFUSION IN Co_3Ti ALLOYS. Acta Metall Sin, 1998, 34(2): 141-145.
|
|
|
Abstract The effect of boron doping on the sensitivity to environmental embrittlement of Co3Ti alloys was investigated. The results show that the boron doping in Co3Ti does not have the effect on suppressing environmental embrittlement. The hydrogen diffusion coefficients in Co3Ti alloys with and without boron measured by a new experimental method have almost the same value, which indicates that boron in Co3Ti alloys does not reduce the hydrogen diffusivity along the grain boundaries. The susceptibility of boron-doped Co3Ti alloys to moisture-induced environmental embrittlement is attributed to no boron atoms segregating to the grain boundaries.
|
|
Received: 18 February 1998
|
1George E P,Liu C T,Pope D P.Scripta Metall,1993;28:875 2 Wan X J, Zhu J H, Jing K L. Scr Metall 1992; 26: 473 3Takasugi,T ,Izumi O.Acta Metall,1986;3:607 4Tasasugi T, Izumi O, Yashida M.J Mater Sci,1991; 26: 1173 5 Wan X J, Zhu J H, Jing K L, Chen W J, Wu Y.J Mater Sci Technol 1994; 10: 39 6万晓景,朱家红,黄胜标.金属学报,1995;31:B183 (Wan X J, Zhu J H, Huang S B、 Acta Metall Sin, 1995; 31: B183) 7Wan X J, Zhu J H, Huang S B. Acta Metall Sin(Eng Lett), 1995; 8: 299 8Liu C T, White C L, Horton J A. Acta Mete 1985; 33: 213 9Wan X J, Zhu J H, Jing K L. Scr Metall Mater 1994; 31: 677 10Takasugi T, Hono K, Suzch S, Hanada S, Sukurai T. Scr Metall , 1993; 29: 1587 11Takasugi T, Takazawa M, Izumi O.J Mater Sci, 1990; 25: 4239 12Zhu J H, Wan X J, Wu Y. Scr Metalll Mater 1993; 29: 429 13George E P,Liu C T.Mat Res Soc Symp Proc,1995; 364:1131` |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|