| COMPUTER SIMULATION ON TEXTURE EVOLUTION OF POLYCRYSTALLINE THIN FILMS DURING GRAIN GROWTH |
| WANG Yandong; LIU Yandong; XU Jiachen; LIANG Zhide(Department of Materials Science and Engineering; Northeastern University;Shenyang 110006) |
|
Cite this article:
WANG Yandong; LIU Yandong; XU Jiachen; LIANG Zhide(Department of Materials Science and Engineering; Northeastern University;Shenyang 110006). COMPUTER SIMULATION ON TEXTURE EVOLUTION OF POLYCRYSTALLINE THIN FILMS DURING GRAIN GROWTH. Acta Metall Sin, 1998, 34(3): 313-318.
|
|
|
Abstract The concept of texture configuration entropy is introduced into the computer simulation on texture evolution of polycrystalline films. The grain orientation distribution in thin films is quantitatively determined by a new simple model. As an example, inverse pole figures of polycrystalline aluminum thin films are simulated by considering the change of texture configuration entropy and another orientation dependent driving forces during grain growth, such as surface energy and strain energy. The physical mechanisms affecting the texture evolution of polycrystalline thin films are discussed.
|
|
Received: 18 March 1998
|
1Carel R, Thompson C V, Frost H J. Acta Mater, 1996; 44: 2479 2Waner F, Lamm L, Deparis D. Textures Microstruct, l995; 23: 249 3Li D Y, Szpunar J. Mater Sci Forum, 1994; 157-162: 1827 4Liu Y D, Wang Y D, Xu J Z, Hu X T. In: Liang Zhide, Zuo Liang eds., Proc 11th Int Coof onTedure of Materiais (ICOTOM-11), Vol.II, Xi'an, 1996: 1165 5Wang F, Xu J Z, Liang Z D. Pme 9th Int Coof on Textures of Materiale(JCOTOM-8), TheMetallurgical Society, Santa Fe, USA, 1987: 110 6王沿东,徐家桢金属学报,1995;31:B550(Wang Yandong, XU Jiazhen. Acta Metall Sin, 1995; 31: B550) 7Wang Y D, Liu Y D, Xu J Z, Liang Z D. J Appl Phys, 1996; 79: 7376 8Wang Y D, Vadon A, Heizmann J J, Xu J Z. Scr Mater, 1996; 35: 905 9陈仁烈统计物理引论北京:人民教育出版社,1959:104(Chen Renlie. The Intnduction Of Statisticnl Physics. Beijing: People's Education Press, 1959: 104) 10Mackenzie J K, Moore A J W, Nicholas J F. i Phys Chem Solids, 1962; 23: 185 11Baskes M I. Phys Rev, 1992; B46: 2727 12Daw M S, Baskes M I. Phys Rev Lett, 1983, 50: 1285 13Klokholm E, Berry B S. J Eletrochem Soc, 1968;115: 823 14Bassett G A, Menter J W, Bashley D W. Proc R Soc London, 1958; A246: 345 15Toth L S, Gilormini P, Jonas J J. Acta Metall, 1988; 36: 3077 16Braun J, Sambridge M. Nature, 1995; 376: 6542 17Li D Y, ffecaniere C, Das S, Szpunar J A. Mater Sci Forvm, 1994; 157-162: 555 |