Please wait a minute...
Acta Metall Sin  2009, Vol. 45 Issue (1): 18-24    DOI:
论文 Current Issue | Archive | Adv Search |
DAMPING CAPACITY AND MECHANICAL PROPERTY OF
NiTiNb SHAPE MEMORY ALLOYS
XIAO Fu1; ZHAO Xinqing1; XU Huibin1;JIANG Haichang2; RONG Lijian2
1 School of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083 
2 Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016
Cite this article: 

XIAO Fu ZHAO Xinqing XU Huibin JIANG Haichang RONG Lijian. DAMPING CAPACITY AND MECHANICAL PROPERTY OF
NiTiNb SHAPE MEMORY ALLOYS. Acta Metall Sin, 2009, 45(1): 18-24.

Download:  PDF(1075KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Two-phase NiTi base alloys (NiTi)50-0.5xNbx (x=5, 10, 15, 20) with both high damping capacity and high yield strength have been prepared by addition of Nb. With increasing Nb content, the fraction of eutectic (NiTi+β--Nb) increases, and yield strength in martensite state rises. When x=15, the yield strength reaches the highest value of 289 MPa. And the alloys also exhibit high damping capacity, tanδ>0.01. According to the damping mechanism for the shape memory alloys, the relationship between the damping properties and temperatures of NiTiNb alloys was explained, and phase boundary damping from the β-Nb and NiTi phases was discussed.

Key words:  NiTiNb shape memory alloy      martensite phase transformation      damping capacity      yield strength     
Received:  21 May 2008     
ZTFLH: 

TG113.22

 
Fund: 

Supported by National High Technology Research and Development Program of China
(No.2006AA03Z102) and Aviation Science Foundation
of China (No.2006ZF51069)

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I1/18

[1] Otsuka K, Ren X. Prog Mater Sci, 2005; 50: 511
[2] Van Humbeeck J. J Alloys Compd, 2003; 355: 58
[3] Cai W, Lu X L, Zhao L C. Mater Sci Eng, 2005; A394: 78
[4] Wu S K, Lin H C. J Alloys Compd, 2003; 355: 72
[5] Cai W, Meng X L, Zhao L C. Curr Opin Solid State Mater Sci, 2005; 9: 296
[6] Xiao F, Ma G J, Zhao X Q, Xu H B, Jiang H C, Rong L J. Proc SPIE, 2007; 6423: 64232L
[7] Rajagopalan S, Little A L, Bourke M A M, Vaidyanathan R. Appl Phys Lett, 2005; 86: 081901
[8] Schaller R. J Alloys Compd, 2003; 355: 131
[9] Piao M, Miyazaki S, Otsuka K, Nishida N. Mater Trans JIM, 1992; 33: 337
[10] Piao M, Miyazaki S, Otsuka K. Mater Trans JIM, 1992; 33: 346
[11] Zhao X Q, Yan X M, Yang Y Z, Xu H B. Mater Sci Eng, 2006; A575: 438
[12] He X M, Rong L J, Yan D S, Li Y Y. Mater Sci Eng, 2004; A371: 193
[13] Bidaux J E, Schaller R, Benoit W. Acta Metall, 1989; 37: 803
[14] San Juan J, No M L. J Alloys Compd, 2003; 355: 65
[15] P´er´ez–Saez R B, Recarte V, No M L, San Juan J. Phys Rev, 1998; 57B: 5684
[16] San Juan J, No M L. Mater Sci Eng, 2006; A442: 429
[17] Ritchie I G, Pan Z L. Metall Trans, 1991; 22A: 607
[18] Xiao F, Zhao X Q, Xu H B, Jiang H C, Rong L J. Chin J Aeronaut, 2009; 22: in press
[19] Melton K N, Mercier O. Acta Metall, 1981; 29: 393

 

[1] SHEN Guohui, HU Bin, YANG Zhanbing, LUO Haiwen. Influence of Tempering Temperature on Mechanical Properties and Microstructures of High-Al-Contained Medium Mn Steel Having δ-Ferrite[J]. 金属学报, 2022, 58(2): 165-174.
[2] WANG Yu, HU Bin, LIU Xingyi, ZHANG Hao, ZHANG Haoyun, GUAN Zhiqiang, LUO Haiwen. Influence of Annealing Temperature on Both Mechanical and Damping Properties of Nb-Alloyed High Mn Steel[J]. 金属学报, 2021, 57(12): 1588-1594.
[3] WANG Shihong, LI Jian, CHAI Feng, LUO Xiaobing, YANG Caifu, SU Hang. Influence of Solution Temperature on γ→ε Transformation and Damping Capacity of Fe-19Mn Alloy[J]. 金属学报, 2020, 56(9): 1217-1226.
[4] Yantao YAO, Liqing CHEN, Wenguang WANG. Damping Capacities of (B4C+Ti) Hybrid Reinforced Mg and AZ91D Composites Processed by In Situ Reactive Infiltration Technique[J]. 金属学报, 2019, 55(1): 141-148.
[5] Xiaofeng HU,Yubin DU,Desheng YAN,Lijian RONG. Cu Precipitation and Its Effect on Damping Capacity and Mechanical Properties of FeCrMoCu Alloy[J]. 金属学报, 2017, 53(5): 601-608.
[6] Rui XIE,Zheng LU,Chenyang LU,Zhengyuan LI,Xueyong DING,Chunming LIU. CHARACTERIZATION OF NANOSIZED PRECIPITATES IN 9Cr-ODS STEELS BY SAXS AND TEM[J]. 金属学报, 2016, 52(9): 1053-1062.
[7] Rui CHEN,Qingyan XU,Baicheng LIU. MODELLING INVESTIGATION OF PRECIPITATION KINETICS AND STRENGTHENING FOR NEEDLE/ROD-SHAPED PRECIPITATES INAl-Mg-Si ALLOYS[J]. 金属学报, 2016, 52(8): 987-999.
[8] Ke ZHANG,Qilong YONG,Xinjun SUN,Zhaodong LI,Peilin ZHAO. EFFECT OF COILING TEMPERATURE ON MICRO-STRUCTURE AND MECHANICAL PROPERTIES OF Ti-V-Mo COMPLEX MICROALLOYED ULTRA-HIGH STRENGTH STEEL[J]. 金属学报, 2016, 52(5): 529-537.
[9] Wei GU,Jingyuan LI,Yide WANG. EFFECT OF GRAIN SIZE AND TAYLOR FACTOR ON THE TRANSVERSE MECHANICAL PROPERTIES OF 7050 ALUMINIUM ALLOY EXTRUSION PROFILE AFTER OVER-AGING[J]. 金属学报, 2016, 52(1): 51-59.
[10] QIN Fei, XIANG Min, WU Wei. THE STRESS-STRAIN RELATIONSHIP OF TSV-Cu DETERMINED BY NANOINDENTATION[J]. 金属学报, 2014, 50(6): 722-726.
[11] WANG Xiaona, HAN Lizhan, GU Jianfeng. PRECIPITATION KINETICS AND YIELD STRENGTH MODEL FOR NZ30K-Mg ALLOY[J]. 金属学报, 2014, 50(3): 355-360.
[12] ZHANG Longfei, YAN Ping, ZHAO Jingchen,HAN Fengkui, ZENG Qiang. ANALYZING THE YIELD STRENGTH OF SUPERALLOY SINGLE CRYSTAL DD407 AT 760℃ BY LCP-MODEL[J]. 金属学报, 2013, 29(4): 489-494.
[13] LIU Gang SUN Yali HU Jin ZHOU Ke. DAMPING CAPACITY OF Bi2O3–COATED Al18B4O33 WHISKER REINFORCED Al MATRIX COMPOSITES[J]. 金属学报, 2010, 46(8): 979-983.
[14] . STRESS--STRAIN BEHAVIORS AROUND THE YIELD STRENGTH IN SEQUENTIAL ROOM TEMPERATURE CREEP TESTS[J]. 金属学报, 2009, 45(7): 840-843.
[15] HU Xiaofeng LI Xiuyan ZHANG Bo RONG Lijian LI Yiyi. INFLUENCES OF ADDITIONS OF Nb, Ti AND Cu ON DAMPING CAPACITY AND CORROSION RESISTANCE OF Fe--13Cr--2.5Mo ALLOY[J]. 金属学报, 2009, 45(6): 717-722.
No Suggested Reading articles found!