Effect of material properties of cold-sprayed particles on its impacting behavior
北京科技大学
Cite this article: 

. Effect of material properties of cold-sprayed particles on its impacting behavior. Acta Metall Sin, 2008, 44(11): 1286-1291 .

Download:  PDF(4407KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The deformation behavior of Cu, Al, Ti alloy and Ni alloy particles upon Cu substrates in cold spraying was studied using the finite element analysis, and effect of material properties of cold-sprayed particles on its impacting behavior. The results indicated that, compared to the substrate, particles with higher effective plastic limit were inclined to undergo adiabatic shear instability. The substrate without adiabatic shear instability released deformation energy, which lead to rebound of particles. Adiabatic shear instability wasn’t observed in particles with lower effective plastic limit, and the release of the deformation energy promoted the adiabatic shear instability of substrate.
Key words:       
Received:  28 April 2008     
ZTFLH:  TG174.442  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I11/1286

[1]Klinkov S V,Kosarev V F,Rein M.Aerosp Sci Technol, 2005;9:582
[2]Alkimov A P,Kosarev V F,Papyrin A N.Dokl Akad Nauk SSSR,1990;315:1062
[3]Alkhimov A P,Kosarev V F,Nesterovich N I,Papyrin A N,Shushpanov M M.Russ Pat,1618778,1990
[4]Assadi H,G(?)rtner F,Stoltenhoff T,Kreye H.Acta Mater, 2003;51:4379
[5]Li W Y,Liao H L,Li C J,Li G,Coddet C,Wang X F. Appl Surf Sci,2006;253:2852
[6]Li W Y,Liao H L,Li C J,Bang H S,Coddet C.Appl Surf Sci,2007;253:5084
[7]Crujicic M,Saylor J R,Beasley D E,DeRosset W S,Hel- fritch D.Appl Surf Sci,2003;219:211
[8]Li W Y,Li C J,Wang Y Y,Yang C J.Acta Metall Sin, 2005;41:282 (李文亚,李长久,王豫跃,杨冠军.金属学报,2005;41:282)
[9]Balani K,Agarwal A,Seal S,Karthikeyan J.Scr Mater, 2005;53:845
[10]G(?)rtner F,Borchers C,Assadi H.In:Marple B,Moreau C, eds.,Proc Int Thermal Spray Conference,Orlando:ASM International,2003:1
[11]van Steenkiste T H,Smith J R,Teets R E.Surf Coat Technol,2002;154:237
[12]Schmidt T,G(?)rtner F,Assadi H,Kreye H.Acta Mater, 2006;54:729
[13]Jodoin B.J Therm Spray Technol,2002;11:496
[14]Jodoin B,Ajdelsztajn L,Sansoucy E,Zuniga A,Richer P, Lavernia E J.Surf Coat Technol,2006;201:3422
[15]Gilmore D L,Dykhuizen R C,Neiser R A,Rocmer T J, Smith M F.J Therm Spray Technol,1999;8:576
[16]Grujicic M,Zhao C L,Tong C,DeRosset W S,Helfritch D.Mater Sci Eng,2004;A368:222
[17]Li C J,Li W Y,Wang Y Y.Thermal Spray 2003:Advanc- ing the Science and Applying the Technology.Materials Park,OH:ASM,2003:9
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!