| Effect of material properties of cold-sprayed particles on its impacting behavior |
| 北京科技大学 |
|
Cite this article:
. Effect of material properties of cold-sprayed particles on its impacting behavior. Acta Metall Sin, 2008, 44(11): 1286-1291 .
|
|
|
Abstract The deformation behavior of Cu, Al, Ti alloy and Ni alloy particles upon Cu substrates in cold spraying was studied using the finite element analysis, and effect of material properties of cold-sprayed particles on its impacting behavior. The results indicated that, compared to the substrate, particles with higher effective plastic limit were inclined to undergo adiabatic shear instability. The substrate without adiabatic shear instability released deformation energy, which lead to rebound of particles. Adiabatic shear instability wasn’t observed in particles with lower effective plastic limit, and the release of the deformation energy promoted the adiabatic shear instability of substrate.
|
|
Received: 28 April 2008
|
|
|
[1]Klinkov S V,Kosarev V F,Rein M.Aerosp Sci Technol, 2005;9:582 [2]Alkimov A P,Kosarev V F,Papyrin A N.Dokl Akad Nauk SSSR,1990;315:1062 [3]Alkhimov A P,Kosarev V F,Nesterovich N I,Papyrin A N,Shushpanov M M.Russ Pat,1618778,1990 [4]Assadi H,G(?)rtner F,Stoltenhoff T,Kreye H.Acta Mater, 2003;51:4379 [5]Li W Y,Liao H L,Li C J,Li G,Coddet C,Wang X F. Appl Surf Sci,2006;253:2852 [6]Li W Y,Liao H L,Li C J,Bang H S,Coddet C.Appl Surf Sci,2007;253:5084 [7]Crujicic M,Saylor J R,Beasley D E,DeRosset W S,Hel- fritch D.Appl Surf Sci,2003;219:211 [8]Li W Y,Li C J,Wang Y Y,Yang C J.Acta Metall Sin, 2005;41:282 (李文亚,李长久,王豫跃,杨冠军.金属学报,2005;41:282) [9]Balani K,Agarwal A,Seal S,Karthikeyan J.Scr Mater, 2005;53:845 [10]G(?)rtner F,Borchers C,Assadi H.In:Marple B,Moreau C, eds.,Proc Int Thermal Spray Conference,Orlando:ASM International,2003:1 [11]van Steenkiste T H,Smith J R,Teets R E.Surf Coat Technol,2002;154:237 [12]Schmidt T,G(?)rtner F,Assadi H,Kreye H.Acta Mater, 2006;54:729 [13]Jodoin B.J Therm Spray Technol,2002;11:496 [14]Jodoin B,Ajdelsztajn L,Sansoucy E,Zuniga A,Richer P, Lavernia E J.Surf Coat Technol,2006;201:3422 [15]Gilmore D L,Dykhuizen R C,Neiser R A,Rocmer T J, Smith M F.J Therm Spray Technol,1999;8:576 [16]Grujicic M,Zhao C L,Tong C,DeRosset W S,Helfritch D.Mater Sci Eng,2004;A368:222 [17]Li C J,Li W Y,Wang Y Y.Thermal Spray 2003:Advanc- ing the Science and Applying the Technology.Materials Park,OH:ASM,2003:9 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|