| A fluctuation electron microscopy study of metallic glasses |
| ;Jianqiang Wang;En Ma |
| 联合 |
|
Cite this article:
Jianqiang Wang; En Ma. A fluctuation electron microscopy study of metallic glasses. Acta Metall Sin, 2008, 44(11): 1388-1393 .
|
|
|
Abstract Al85Ni5Y10-xCox (x = 0, 2) and Cu46Zr54-xAlx (x = 0, 7) metallic glasses (MGs) have been examined using fluctuation electron microscopy (FEM). Strong medium-range order (MRO) was revealed in both MG systems, by peaks in intensity variance curves. Minor changes in composition result in differences in these peaks, while diffraction patterns remain identical. Specifically, minor alloyings of Co into the Al85Ni5Y10 and Al into the Cu46Zr54, forming Al85Ni5Y8Co2 and Cu46Zr47Al7 MGs, render the medium-range structure more homogeneous. This is in a good agreement with the increase of glass-forming ability in the two systems. This result sheds light on FEM as a useful tool to totally sense the structural changes in the medium range, helpful to study the effect of sample composition on properties of metallic glasses.
|
|
Received: 07 May 2008
|
|
|
[1]Wang W H.Prog Mater Sci,2007;52:540 [2]Treacy M M J,Gibson J M.Acta Cryst,1996;52A:212 [3]Hufnagel T C.Nature Mater,2004;3:666 [4]Teacy M M J,Gibson J M,Fan L,Paterson D G,McNulty I.Rep Prog Phys,2005;68:2899 [5]Inoue A,Matsumoto N,Masumoto T.Mater Trans JIM, 1990;31:493 [6]Xu D H,Duan G,Johnson W L.Phys Rev Lett,2004;92: 245504 [7]Wang D,Tan H,Li Y.Acta Mater,2005;53:2969 [8]Yu P,Bai H Y,Tang M B,Wang W L.J Non-Cryst Solids, 2005;351:1328 [9]Kumar G,Ohkubo T,Mukai T,Hono K.Scr Mater,2007; 57:173 [10]Park K W,Jang J,Wakeda M,Shibutani Y,Lee J C.Scr Mater,2007;57:805 [11]Rudee M L,Howie A.Philo Mag,1972;25:1001 [12]Chaudhari P,Graczyk J F,Charbnau H P.Phys Rev Lett, 1972;29:425 [13]Voyles P M.PhD Dissertation,University of Illinois at Urbana-Champaign,Urbana,2000 [14]Wen J,Yang H W,Guo H,Wu B,Sui M L,Wang J Q, Ma E.J Phys:Condens Matter,2007;19:455211 [15]Stratton W G,Hamann J,Perepezko J H,Voyles P M, Mao X,Khare S V.Appl Phys Lett,2005;86:141910 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|