Hydrogen evolution reaction on the composite LaNi5/Ni-S alloy film in alkaline medium
;;;
东北大学
Cite this article: 

;. Hydrogen evolution reaction on the composite LaNi5/Ni-S alloy film in alkaline medium. Acta Metall Sin, 2008, 44(7): 887-891 .

Download:  PDF(887KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By molten salt electrolysis combined with aquatic electrodeposition, the composite LaNi5/Ni-S film with high stability and HER activity was obtained. The results showed that in the Na3AlF6-La2O3 (92 : 8) molten salt system, although the cathodic potential is much lower than the decomposition potential of lanthanum, the LaNi5 film could be obtained due to the strong depolarization ability of Ni cathode. The composite LaNi5/Ni-S film (η150 = 75 mV, 80oC) could absorb large amount of H atoms, which would be oxidized and avoid the dissolution of the Ni-S film under the state of open-circuit effectively and prolong the lifetime of the cathode.
Key words:       
Received:  14 December 2007     
ZTFLH:  TF123.1  
  TG146  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I7/887

[1]Norsk H.Netherlands Pat,7801955,1978
[2]Hine F,Yasuda M,Watanabe M.Denki Kagaku,1979;47: 401 (日根富郎,安田正雄,渡边正男.电气化学,1979;47:401)
[3]Gonsalez E R,Avaca L A,Tremiliosi-Filho G.Int J Hy- drogen Energy,1994;19:17
[4]Sabela R,Paseka I.J Appl Electrochem,1990;20:500
[5]Paseka I.Electrochim Acta,1993;38:2449
[6]de Giz M J,Ferreira M,Gonzalez E R.J Appl Electrochem, 1993;23:641
[7]Vandenborre H,Vermeiren Ph,Leysen R.Electrochim Acta,1984;29:297
[8]Wen T C,Lin S M,Tsai J M.J Appl Electrochem,1994; 24:233
[9]Valand T,Burchardt T,Grontoft T.Int J Hydrogen En- ergy,2002;27:39
[10]Xu Y H,He G R,Wang X L.Int J Hydrogen Energy,2003; 28:961
[11]Kitamura T,Iwakura C,Tamura H.Chem Left,1981:965
[12]Kitamura T,Iwakura C,Tamura H.Chem Left,1981:1755
[13]Hu W K.Int J Hydrogen Energy,2000;25:111
[14]Bocutti R,Saeki M J,Florentino A O.Int J Hydrogen Energy,2000;25:1051
[15]Han Q,Liu K R,Chen J S.Int J Hydrogen Energy,2003; 28:1207
[16]Bard A J,Fauikner L R.Electrochemical Methods Fun- damentals and Applications.2nd Ed.,New York:John Wiley & Sons,INC,2003:135
[17]Carvalho J D,Tremiliosi-Filho G,Avaca L A.In:Srini- vasan S,Wagner S,Wroblowa H,eds.,Electrode Materials and Processes .for Energy Conversion and Storage.Pen- nington:The Electrochem Soc Inc,1987:356
[18]Vandenborre H,Vermeiren P,Leysen R.Electrochim Acta, 1984;29:297
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!