| A study on the Silicon reactivity in the galvanizing |
| SU Xu-Ping;Zhi LI;Fucheng YIN;Shiwen Pan |
| 湘潭大学机械工程学院;材料设计及制备技术湖南省重点实验室 |
|
Cite this article:
SU Xu-Ping; Zhi LI; Fucheng YIN; Shiwen Pan. A study on the Silicon reactivity in the galvanizing. Acta Metall Sin, 2008, 44(6): 718-722 .
|
|
|
Abstract According to the thermodynamic calculation of the Zn-Fe-Si ternary phase system and experimental investigation, the chemical potential of Si increases greatly with the Zn content. So the Si in the coating trends to gather in the high Fe content phases such as the phase near the / phase boundary, the phase boundary of the / layer and the crystal boundary of the phase. A model was proposed. In galvanizing, diffusion path in coating becomes Si rich, Si concentration in the crystal boundary of the increases. Diffusion path cut the Tieline of the +Liquid Zn phase equilibrium, and liquid phase appears in the crystal boundary of phase. Liquid channels Crosse the layer, connect with the outside liquid Zn. Liquid channel also contacts with the phase. The Diffuse- (cracked phase+Liquid Zn) region forms. Since the liquid attacks substrate directly, the growth of coating is reaction controlled. The coating grows linearly.
|
|
Received: 12 September 2007
|
|
|
[1]Sandelin R W.Wire Wire Prod,1940;15:3 [2]Guttman H,Niessen P.Can Metall Quart,1972;11:609 [3]Devillers L P,Guttman H,Niessen P.Proc Galvanization Si Containing Steels,Liege:ILZRO Publ.,1975:48 [4]Pearce D C.ASARCO Res Rep,1974:4659 [5]Pclcrin J.PhD Thesis,Universit■des Sciences et Tech- niques de Lille,Paris,1983 [6]Habraken L.Proc 12th Int Galvanizing Conf,Paris: Portcullis Press Ltd.,1979:121 [7]Kozdras M S,Nissen P.Metallography,1989;22:253 [8]Foct J,Perrot P,Reumont G.Scr Metall Mater,1993;28: 1195 [9]Bretez M,Dauphin J Y,Foct J,Perrot P.Z Metallkd, 1987;78:137 [10]Perrot P,Dauphin J Y.Calphad,1988;12:33 [11]Leprctre Y,Mataigne J M.In:Prank E G ed.,Zn-Based Steel Coating Systems:Production and Performance,San Antonio:TMS,1998:303 [12]KSster W.Metallurgia,1969;80:219 [13]Uwakweh O,Jordan A.J Phase Equilib,1997;18:448 [14]Raghavan V.Phase Diagram of Ternary Iron Alloys.Part 6,New Delhi:Indian Institute of Metals,1992:1183 [15]Su X,Tang N,Toguri J.Can Metall Quart,2001;40:377 [16]Su X,Yin F,Li Z,Tang N,Zhao M.J Alloy Compd,2005; 396:156 [17]Sundman B,Janson B,Andersson J O.Calphad,1985;9: 153 [18]Su X,Tang N,Toguri J.J Alloy Compd,2001;325:129 [19]Lu J,Che C,Kong G,Xu Q,Chen J.Surf Coat Technol, 2006;200:5277 [20]Hong M H,Saka H.Acta Mater,1997;45:4225m |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|