Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (6): 718-722     DOI:
Research Articles Current Issue | Archive | Adv Search |
A study on the Silicon reactivity in the galvanizing
SU Xu-Ping;Zhi LI;Fucheng YIN;Shiwen Pan
湘潭大学机械工程学院;材料设计及制备技术湖南省重点实验室
Cite this article: 

SU Xu-Ping; Zhi LI; Fucheng YIN; Shiwen Pan. A study on the Silicon reactivity in the galvanizing. Acta Metall Sin, 2008, 44(6): 718-722 .

Download:  PDF(773KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  According to the thermodynamic calculation of the Zn-Fe-Si ternary phase system and experimental investigation, the chemical potential of Si increases greatly with the Zn content. So the Si in the coating trends to gather in the high Fe content phases such as the  phase near the / phase boundary, the phase boundary of the  /  layer and the crystal boundary of the  phase. A model was proposed. In galvanizing, diffusion path in coating becomes Si rich, Si concentration in the crystal boundary of the  increases. Diffusion path cut the Tieline of the +Liquid Zn phase equilibrium, and liquid phase appears in the crystal boundary of  phase. Liquid channels Crosse the  layer, connect with the outside liquid Zn. Liquid channel also contacts with the  phase. The Diffuse- (cracked  phase+Liquid Zn) region forms. Since the liquid attacks substrate directly, the growth of coating is reaction controlled. The coating grows linearly.
Key words:       
Received:  12 September 2007     
ZTFLH:  TG111.3  
  TG111.5  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I6/718

[1]Sandelin R W.Wire Wire Prod,1940;15:3
[2]Guttman H,Niessen P.Can Metall Quart,1972;11:609
[3]Devillers L P,Guttman H,Niessen P.Proc Galvanization Si Containing Steels,Liege:ILZRO Publ.,1975:48
[4]Pearce D C.ASARCO Res Rep,1974:4659
[5]Pclcrin J.PhD Thesis,Universit■des Sciences et Tech- niques de Lille,Paris,1983
[6]Habraken L.Proc 12th Int Galvanizing Conf,Paris: Portcullis Press Ltd.,1979:121
[7]Kozdras M S,Nissen P.Metallography,1989;22:253
[8]Foct J,Perrot P,Reumont G.Scr Metall Mater,1993;28: 1195
[9]Bretez M,Dauphin J Y,Foct J,Perrot P.Z Metallkd, 1987;78:137
[10]Perrot P,Dauphin J Y.Calphad,1988;12:33
[11]Leprctre Y,Mataigne J M.In:Prank E G ed.,Zn-Based Steel Coating Systems:Production and Performance,San Antonio:TMS,1998:303
[12]KSster W.Metallurgia,1969;80:219
[13]Uwakweh O,Jordan A.J Phase Equilib,1997;18:448
[14]Raghavan V.Phase Diagram of Ternary Iron Alloys.Part 6,New Delhi:Indian Institute of Metals,1992:1183
[15]Su X,Tang N,Toguri J.Can Metall Quart,2001;40:377
[16]Su X,Yin F,Li Z,Tang N,Zhao M.J Alloy Compd,2005; 396:156
[17]Sundman B,Janson B,Andersson J O.Calphad,1985;9: 153
[18]Su X,Tang N,Toguri J.J Alloy Compd,2001;325:129
[19]Lu J,Che C,Kong G,Xu Q,Chen J.Surf Coat Technol, 2006;200:5277
[20]Hong M H,Saka H.Acta Mater,1997;45:4225m
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!