EFFECT OF ALLOYING ELEMENTS ON THE FORMATION AND STRUCTURAL FEATURES OF LONG PERIOD STACKING STRUCTURES IN AS-SOLIDIFIED MG ALLOYS
北京工业大学
Cite this article: 

. EFFECT OF ALLOYING ELEMENTS ON THE FORMATION AND STRUCTURAL FEATURES OF LONG PERIOD STACKING STRUCTURES IN AS-SOLIDIFIED MG ALLOYS. Acta Metall Sin, 2008, 44(4): 428-432 .

Download:  PDF(1152KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Mg97Y2X1(at%,X= Zn,Ni,Ag)alloys were prepared by induction melting method and characteristic long period stacking structures(LPS) formed in these alloys studied by transmission electron microscopy and scanning electron microscopy. The results show that the LPS in the as-solidified Mg97Y2Zn1 can be described as a structure with a 6-layer stacking period, which is different from the typical LPS of the 6H type in a hcp structure. The existence of LPS in the Mg-Y-Ni system has been found for the first time. The lattice distortion in LPS structures occurs more often in the Mg-Y-Ni system than in the Mg-Y-Zn system. In contrast, no LPS structure is found to be formed in the Mg-Y-Ag sysyem. On the basis of experimental results, the factors affecting the formation of LPS structures in Mg97Y2X1 alloys are also discussed.
Key words:       
Received:  17 May 2007     
ZTFLH:  TG146.4  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I4/428

[1]Kawamura Y,Hayashi K,Inoue A,Masumoto T.Mater Trans,2001;42:1172
[2]Itoi T,Kawamura Y,Hirohashi M.Scr Mater,2004;51: 107
[3]Amiya K,Ohsuna T,Inoue A.Mater Trans,2003;44: 2151
[4]Abe E,Kawamura Y,Haysshi K,Inoue A.Acta Mater, 2002;50:3845
[5]Inoue A,Matsushita M,Kawamura Y,Amiya K,Hayashi K,Koike J.Mater Trans,2002;43:580
[6]Kawamura Y,Kasahara T,Izumi S,Yamasaki M.Scr Mater,2006;55:453
[7]Takeuchi A,Inoue A.Mater Trans,2005;46:2817
[8]Datta A,Ramamurty U,Ranganathan S,Waghmare U V. Comput Mater Sci,2006;37:69
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!