| EFFECTS OF ALLOY COMPOSITION AND PROCESS PARAMETERS ON THE HEAT TRANSFER COEFFICIENT AT METAL/DIE INTERFACE IN HIGH PRESSURE DIE CASTING |
| ;;Sang-Hyun CHO; |
| 北京清华大学机械工程系 |
|
Cite this article:
Sang-Hyun CHO. EFFECTS OF ALLOY COMPOSITION AND PROCESS PARAMETERS ON THE HEAT TRANSFER COEFFICIENT AT METAL/DIE INTERFACE IN HIGH PRESSURE DIE CASTING. Acta Metall Sin, 2008, 44(4): 433-439 .
|
|
|
|
|
Received: 27 September 2007
|
|
|
[1]Ho K,Pehlke R D.Metall Trans,1985;16B:585 [2]Pehlke R D.In:Cross M,Campbell J,eds.,Proc 1995 7th Conf on Modeling of Casting,Welding and Advanced Solidification Processes,London:Minerals,Metals & Ma- terials Soc(TMS),1995:373 [3]Guthrie R I L,Isac M,Kim J S,Tavares R P.Metall Mater Trans,2000;31B:1031 [4]Hallam C P,Griffiths W D,Butler N D.Mater Sci Forum, 2000;329-330:467 [5]Krishnan M,Sharma D G R.Trans Am Foundrymen's Soc,1995;102:769 [6]Muojekwu C A,Samarasekera I V,Brimacombe J K.Met- all Mater Trans,1995;26B:361 [7]Gozlan E,Bamberger M.Z Metallkd,1987;78:677 [8]El-Mahallawy N A,Assar A M.J Mater Sci Lett,1988; 7:205 [9]Nishida Y,Matsubara H.Br Foundryman,1976;69:274 [10]Davies V.Br Foundryman,1980;73:331 [11]Sekhar J A,Abbaschian G J,Mehrabian R.Mater Sci Eng,1979;40:105 [12]Bamberger M,Weiss B Z,Stupel M M.Mater Sci Technol, 1987;3:49 [13]Santos C A,Quaresma J M V,Garcia A.J Alloys Compd, 2001;319:174 [14]Hallam C P,Griffiths W D.Metall Mater Trans,2004; 35B:721 [15]Chiesa F.Trans Am Foundrymen's Soc,1990;98:193 [16]Coates B,Argyropoulos S A.Metall Mater Trans,2007; 38B:243 [17]Dour G,Dargusch M,Davidson C.Int J Heat Mass Trans- fer,2006;49:1773 [18]Guo Z P,Xiong S M,Cho S-H,Choi J-K.Acta Metall Sin,2007;43:607 (郭志鹏,熊守美,曺尚铉,崔正吉.金属学报,2007;43:607) [19]Nelson C W.In:SDCE,ed.,Transaction of 6th Inter- national Die Casting Congress & Exhibition,Cleveland, OH:SDCE,1970:1 [20]Hong S,Backman D G,Mehrabian R.Metall Mater Trans, 1979;10B:299 [21]Papai J,Mobley C.In:NADCA ed.,Transactions of the NADCA Congress,Detroit,MI:NADCA,1991:377 [22]Dour G,Dargusch M,Davidson C,Nef A.J Mater Process Technol,2005;169:223 [23]Beck J V.J Heat Transfer,Trans ASME,1977;99C:314 [24]Michalski L,Echersdort K,McGhee J.Temperature Mea- surement.New York:Wiley,1991:252. [25]Helenius R,Lohne O,Arnberg L,Laukli H I.Mater Sci Eng,2005;A413-414:52 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|