Export:  BibTeX | EndNote (RIS)      
Abstract  Microstructures and mechanical properties of AZ91 magnesium alloy after homogenized, hot extrusion and succedent aging are investigated. The results show that dynamic recrystallization occurs during extrusion at elevated temperatures of 320℃ and 380℃; compared to the as-cast alloy, microstructures of the extruded AZ91 alloy are refined, and the mechanical properties are enhanced remarkably; succedent aging is helpful to improvement of mechanical properties of the extruded AZ91 alloy. In this experiment, the ultimate tensile strength of the AZ91 alloy extruded at 380℃and aged at 200℃×10h is about 357MPa, and the elongation of the alloy reaches about 8%.
Key words:       
Received:  26 December 2006     
ZTFLH:  TG376.2  
  TG156.92  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I9/920

[1]Mordike B L,Ebert T.Mater Sci Eng,2001;A302:37
[2]Friedrich H,Schumann S.J Mater Process Technol,2001; 117:276
[3]Matucha K H.In:Cahn R W,Hassen P,Kramer E J, eds.;translated by Ding D Y,et al.,Materials Science and Technology:A Comprehensive Treatment,Vol.8:Struc- ture and Properties of Nonferrous Alloys,Beijing:Science Press,1999:105 (Matucha K H.见:Cahn R W,Hassen P,Kramer E J,主编;丁道云,等,译.材料科学与技术丛书,第8卷:非铁合金的结构和性能,北京:科学出版社,1999:105)
[4]Watanabe H,Tsutsui H,Mukai T,Kohzu M,Tanabe S, Higashi K.Int J Plast,2001;17:387
[5]Aghion E,Bronfin B,Eliezer D.J Mater Process Technol, 2001;117:381
[6]Kleiner S,Beffort O,Wahlen A,Uggowitzer P J.J Light Met,2002;2:277
[7]Cizek L,Greger M,Pawlica L,Dobrzanski L A,Tanski T. J Mater Process Technol,2004;157-158:466
[8]Liu Z,Liu C Y,Wang Z G,Wang Y,Han X L.Acta Metall Sin,1999;35:869 (刘正,刘重阳,王中光,王越,韩行林.金属学报,1999;35:869)
[9]Mabuchi M,Kubota K,Higashi K.Mater Trans JIM, 1995;36:1249
[10]Yu BY,Bao C L,Song H W,Qiao R J,Liu Z,Yu H P. Hot Work Technol,2005;34(8):30 (于宝义,包春玲,宋鸿武,乔日金,刘正,于海朋.热加工工艺,2005;34(8):30)
[11]Jin J B,Wang Z X,Liu X F,Xie J X.Acta Metall Sin, 2006;42:1014 (金军兵,王智祥,刘雪峰,谢建新.金属学报,2006;42:1014)
[12]Ion S E,Humphreys F J,White S H.Acta Metall,1982; 30:1909
[13]Mao W M,Zhao X B.Recrystallization and Grain Growth of Metals.Beijing:Metallurgical Industry Press,1994:47 (毛卫民,赵新兵.金属的再结晶与晶粒长大.北京:冶金工业出版社,1994:47)
[14]Duly D,Simon J P,Brechet Y.Acta Metall Mater,1995; 43:101
[15]Celotto S.Acta Mater,2000;48:1775
[16]Kubota K,Mabuchi M,Higashi K.J Mater Sci,1999;34: 2255
[17]Wang L Y,Huang G S,Fan Y G,Huang G J.Chin J Nonferrous Met,2003;13:594 (汪凌云,黄光胜,范永革,黄光杰.中国有色金属学报,2003;13:594)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!