| The distribution and diffusion of carbon atoms during deformation of undercooled austenite in medium carbon steel |
| 北京科技大学 |
|
Cite this article:
. The distribution and diffusion of carbon atoms during deformation of undercooled austenite in medium carbon steel. Acta Metall Sin, 2007, 43(8): 785-790 .
|
|
|
Abstract The distribution and diffusion of carbon atoms during deformation of undercooled austenite in the medium carbon steel were investigated by means of uniaxial hot compression simulation experiment and SEM, XRD, thermomagnetic methods. The experimental results showed that the effective diffusion coefficient of the carbon atoms during dynamic transformation of undercooled austenite increased significantly compared with that during the isothermal transformation at the same temperature, as a result the completion of ferrite and pearlite transformation was shortened. During the subsequent spheroidization process of lamellae pearlite, high density dislocations and vacanies introduced during hot deformation promoted the diffusion of the carbon atoms, therefore the cementite spheroidization kinetics was accelerated dramatically as compared to isothermal annealing treatment. The dissolution, re-precipitation of cementite and supersaturated carbon inside the ferrite grains were confirmed. The supersaturated carbon atoms were not located at interstitial sites within the iron lattices homogeneously, but highly segregated in ferrite grain boundaries and dislocation cores.
|
|
Received: 30 October 2006
|
|
|
[1]Shin D H,Park K T,Kim Y S.Scr Mater,2003;48:469 [2]Shin D H,Kim B C,Park K T,Kim Y S.Acta Mater, 2000;48:2247 [3]Song R,Ponge D,Raabe D,Kaspar R.Acta Mater,2005; 53:845 [4]Storojeva L,Ponge D,Kaspar R, Raabe D.Acta Mater, 2004;52:2209 [5]Ivanisenko Y,Lojkowski W,Valiev R Z,Fecht H J.Acta Mater,2003;51:5555 [6]Furuhara T,Mizoguchi T,Maki T.ISIJ Int,2005;45:392 [7]Yaag W Y,Qi J J,Sun Z Q,Yang P.Acta Metall Sin, 2004;40:135 (杨王玥,齐俊杰,孙祖庆,杨平.金属学报,2004;40:135) [8]Chen G A,Yang W Y,Sun Z Q.Acta Metall Sin,2007; 43:27 (陈国安,杨王玥,孙祖庆.金属学报,2007;43:27) [9]Gavriljuk V G.Mater Sci Eng,2003;A345:81 [10]Yu Y N.The Principle of the Metallorgy.Beijing:Metal- lurgical Industry Press,2000:169 (余永宁.金属学原理.北京:冶金工业出版社,2000:169) [11]van Leeuwen Y,Sietsma J,van der Zwaag S.ISIJ Int, 2003;43:767 [12]Li S T.The Experimental Method of X-ray Diffraction. Beijing:Metallurgical Industry Press,1993:56 (李树棠.X射线衍射实验方法.北京:冶金工业出版社,1993:56) [13]Rice J K,Wang J.Mater Sci Eng,1989;A107:23 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|