Ultra-high cycle fatigue behavior of Ti-6Al-4V alloy
ZUO Jinghui; WANG Zhongguang; HAN Enhou
Environmental Corrosion Center; Institute of Metal Research; Chinese Academy of Sciences
Cite this article: 

ZUO Jinghui; WANG Zhongguang; HAN Enhou. Ultra-high cycle fatigue behavior of Ti-6Al-4V alloy. Acta Metall Sin, 2007, 43(7): 705-709 .

Download:  PDF(1112KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:  Ultra-high cycle      
Received:  16 November 2006     
ZTFLH:  TG111.8  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I7/705

[1]Li X W,Xia S Y,Sha A X.Acta Metall Sin,2002;38(增刊):S277 (李兴无,夏绍玉,沙爱学.金属学报,2002,38(Suppl.):S277)
[2]Tobler R L.ASTM STP 601,1976:346
[3]Williams 3 C,Starke E A.Acta Mater,2003;51:5775
[4]Bathias C.Fatigue Fract Eng Mater Struct,1999;22:559
[5]Bathias C,Drouillac L,le Francois P.Int J Fatigue,2001; 23:143
[6]Yang Z G,Li S X,Zhang J M,Zhang J F,Li G Y,Li Z B,Hui W J,Weng Y Q.Acta Mater,2004;52:5235
[7]Cao W D,Zhou Y G.Acta Metall Sin,2002;1273 (曹卫东,周义刚.金属学报,2002,38:1273
[8]Eylon D,Pierce C M.Metall Tran,1976;7A:111
[9]Papakyriacou M,Mayer H,Pyper C,Plenk H,Stanzl- Tschegg S E.Mater Sci Eng,2001;A308:143
[10]Shu D L.Mechanical Performance of Metals.Beijing: China Mathine Press,1995:19 (束德林.金属力学性能.北京:机械工业出版社,1995:19)
[11]Ritchie R O,Boyce B L,Campbell J P,Roder O,Thomp- son A W,Milligan W W.Int J Fatigue,1999;21:653
[12]Morrissey R J,Mcdowell D L,Nicholas T.Int J Fatigue, 1999;21:679
[13]Wang Q Y,Beard J Y,Dubarre A,Baudry G,Rathery S, and Bathias C.Fatigue Fracture Eng Mater Struct,1999, 22:667
[14]Morrissey R J.Nicholas T.Int J Fatigue,2006;28:1577
[15]Morrissey R J,Nicholas T.Int J Fatigue,2005,27:1608
[16]Tens A,Hoffelner W,Duerig T W,Allison J E.Scr Metall, 1983;17:601
[17]Osamu Umezawa,Kotobu Nagai.ISIJ Int,1997;37:1170
[18]Ravichandran K S.Acta Metall Mater,1991;39:401
[19]Nalla R K,Boyce B L,Campbell J P,Peters J O,Ritchie R O.Metall Mater Trans,2002;33A:899
[20]Eylon D.J Mater Sci,1979;14:345B
[1] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[2] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[3] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[4] PAN Fusheng, JIANG Bin. Development and Application of Plastic Processing Technologies of Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1362-1379.
[5] LAN Liangyun, KONG Xiangwei, QIU Chunlin, DU Linxiu. A Review of Recent Advance on Hydrogen Embrittlement Phenomenon Based on Multiscale Mechanical Experiments[J]. 金属学报, 2021, 57(7): 845-859.
[6] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[7] ZHOU Hongwei, BAI Fengmei, YANG Lei, CHEN Yan, FANG Junfei, ZHANG Liqiang, YI Hailong, HE Yizhu. Low-Cycle Fatigue Behavior of 1100 MPa Grade High-Strength Steel[J]. 金属学报, 2020, 56(7): 937-948.
[8] XU Wei,HUANG Minghao,WANG Jinliang,SHEN Chunguang,ZHANG Tianyu,WANG Chenchong. Review: Relations Between Metastable Austenite and Fatigue Behavior of Steels[J]. 金属学报, 2020, 56(4): 459-475.
[9] Changshuai WANG,Lili GUO,Liying TANG,Rongcan ZHOU,Jianting GUO,Lanzhang ZHOU. Oxidation Behavior of GH984G Alloy in Steam at 700 ℃[J]. 金属学报, 2019, 55(7): 893-901.
[10] Jian PENG,Yi GAO,Qiao DAI,Ying WANG,Kaishang LI. Fatigue and Cycle Plastic Behavior of 316L Austenitic Stainless Steel Under Asymmetric Load[J]. 金属学报, 2019, 55(6): 773-782.
[11] Zhefeng ZHANG, Rui LIU, Zhenjun ZHANG, Yanzhong TIAN, Peng ZHANG. Exploration on the Unified Model for Fatigue Properties Prediction of Metallic Materials[J]. 金属学报, 2018, 54(11): 1693-1704.
[12] TAN Meilin, WANG Changshuai, GUO Yongan, GUO Jianting, ZHOU Lanzhang. INFLUENCE OF Ti/Al RATIOS ON γ′ COARSENING BEHAVIOR AND TENSILE PROPERTIES OF GH984G ALLOY DURING LONG-TERM THERMAL EXPOSURE[J]. 金属学报, 2014, 50(10): 1260-1268.
[13] . INFLUENCE OF Ti/Al RATIOS ON γ′ COARSENING BEHAVIOR AND MECHANICAL PROPERTIES OF GH984G DURING LONG-TERM AGING[J]. 金属学报, 0, 0(0): 0-0.
[14] NIE Defu ZHAO Jie ZHANG Junshan. AN APPROACH TO ESTIMATE ROOM TEMPERATURE CREEP OF STRUCTURAL STEELS[J]. 金属学报, 2011, 47(2): 179-184.
[15] QIAN Gui'an HONG Youshi. EFFECTS OF ENVIRONMENTAL MEDIA ON HIGH CYCLE AND VERY-HIGH-CYCLE FATIGUE BEHAVIORS OF STRUCTURAL STEEL 40Cr[J]. 金属学报, 2009, 45(11): 1356-1363.
No Suggested Reading articles found!