| Investigation on the Micro-Deformation Characteristics of Porous NiTi Shape Memory Alloy Using Sem Moire Method |
| JIANG Haichang1); DU Hua2);XIE Huimin2); RONG Lijian1) |
| 1) Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 2) Department of Engineering and Mechanics; Tsinghua University; Beijing 100084 |
|
Cite this article:
JIANG Haichang; DU Hua; XIE Huimin; RONG Lijian. Investigation on the Micro-Deformation Characteristics of Porous NiTi Shape Memory Alloy Using Sem Moire Method. Acta Metall Sin, 2006, 42(11): 1153-1157 .
[1] Kishimoto S, Egashira M, Shinya N. J Soc Mater Sci Jpn, 1991; 40: 637 (岸本哲,江头满,新谷纪雄.材料科学, 1991;40:673) [2] Li B Y, Rong L J, Li Y Y, Gjunter V E. Acta Mater, 2000; 48: 3895 [3] Itin V I, Gjunter V E, Shabalovskaya S A, Sachdeva R L C. Mater Charact, 1994; 32: 179 [4] Chu C L, Chung J C, Chu P K. Trans Nonferrous Met Soc Chin, 2006; 16: 49 [5] Li Y H, Rong L J, Li Y Y. J Alloys Compd, 2002; 345: 271 [6] Li Y H. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2003 (李永华.中国科学院金属研究所博士学位论文,沈阳, 2003) [7] Otsuka K, Waman C M. Shape Memory Materials. Cambridge, UK: Cambridge University Press, 1998: 49 [8] Shang H X, Xie H M, Dai F L, Wang X S. Opt Technol, 2003; 29: 5 (尚海霞,谢惠民,戴福隆,王习术.光学技术,2003;29:5) [9] Gibson L J, Ashby M F. Cellular Solids: Structure and properties. Cambridge, UK: Cambridge University Press, 1997: 159 [10] Gibson L J. J Biomechanisc, 1985; 18: 317 |
| No Suggested Reading articles found! |
|
|