Investigation on the Micro-Deformation Characteristics of Porous NiTi Shape Memory Alloy Using Sem Moire Method
JIANG Haichang1); DU Hua2);XIE Huimin2); RONG Lijian1)
1) Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 2) Department of Engineering and Mechanics; Tsinghua University; Beijing 100084
Cite this article: 

JIANG Haichang; DU Hua; XIE Huimin; RONG Lijian. Investigation on the Micro-Deformation Characteristics of Porous NiTi Shape Memory Alloy Using Sem Moire Method. Acta Metall Sin, 2006, 42(11): 1153-1157 .

Download:  PDF(864KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  24 April 2006     
ZTFLH:  TB381  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I11/1153

[1] Kishimoto S, Egashira M, Shinya N. J Soc Mater Sci Jpn, 1991; 40: 637 (岸本哲,江头满,新谷纪雄.材料科学, 1991;40:673)
[2] Li B Y, Rong L J, Li Y Y, Gjunter V E. Acta Mater, 2000; 48: 3895
[3] Itin V I, Gjunter V E, Shabalovskaya S A, Sachdeva R L C. Mater Charact, 1994; 32: 179
[4] Chu C L, Chung J C, Chu P K. Trans Nonferrous Met Soc Chin, 2006; 16: 49
[5] Li Y H, Rong L J, Li Y Y. J Alloys Compd, 2002; 345: 271
[6] Li Y H. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2003 (李永华.中国科学院金属研究所博士学位论文,沈阳, 2003)
[7] Otsuka K, Waman C M. Shape Memory Materials. Cambridge, UK: Cambridge University Press, 1998: 49
[8] Shang H X, Xie H M, Dai F L, Wang X S. Opt Technol, 2003; 29: 5 (尚海霞,谢惠民,戴福隆,王习术.光学技术,2003;29:5)
[9] Gibson L J, Ashby M F. Cellular Solids: Structure and properties. Cambridge, UK: Cambridge University Press, 1997: 159
[10] Gibson L J. J Biomechanisc, 1985; 18: 317
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!