THE RESEACH ON METAL FLOW DURING EXTRUDING PROCESS UNDER DIFFERENT FRICTION CONDITIONS BY DEFORMING AREA DIVISIO
LI Feng
哈尔滨工业大学
Cite this article: 

LI Feng. THE RESEACH ON METAL FLOW DURING EXTRUDING PROCESS UNDER DIFFERENT FRICTION CONDITIONS BY DEFORMING AREA DIVISIO. Acta Metall Sin, 2007, 43(2): 199-204 .

Download:  PDF(329KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In order to investigate the metal flow behavior during extrusion process with active friction, numerical simulations and experiments were employed to investigate the mechanical mechanism of the extrusion process with active friction. The characteristic quantity such as the second invariant of the deviatoric stress tensor (J2)、Lode parameter( ) were employed for the division of deformation area. The results show that when extruding with active friction, no metal flow interface forms at the container bottom, the dead metal zone completely disappears, the deformation type of the metal in the plastic deformation area changes from three to the tension type, and the homogeneity of the deformation as well as metal flow is greatly improved. Therefore, it will be easy for extruding and promoting the extrudates quality.
Key words:       
Received:  05 June 2006     
ZTFLH:  TG376  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I2/199

[1]Shan D B,Xu W C,Lu Y.J Mater Process Technol,2004;151:289
[2]Hsu T C,Huang C C.J Mater Process Technol,2003;140:49
[3]Tan X C.Int Tribol,2002;35:385
[4]Lin Z P,Hua J.J Nanchang Univ,1988;10(1):20(林治平,花江.南昌大学学报.1988;10(1):20)
[5]Miiller K B.In:Kiuchi M,Nishimura H,Yanagimoto J,eds.,Advanced Technology of Plasticity 2002,Pvoc 7th ICTP,Japan,2002:427
[6]He Z B,Hu W L,Wang Z R.In:Bariani P Fed,Advanced Technology of Plasticity 2005,Proc 8th ICTP,Verona,Italy:Edizioni Progetto Padova,2005:407
[7]Wang Z R.Fundamental of Plastic Working Mechanics.Beijing:National Defence Industry Press,1989:127(王仲仁.塑性加工力学基础.北京:国防工业出版社,1989:127)
[8]Hu W L,He Z B,Fang Y.J Mater Process Technol,2004;151:27
[9]He Z B.PhD Dissertation,Harbin Institute of Technology,2005(何祝斌.哈尔滨工业大学博士学位论文,2005)
[10]Li F,Yuan S J,Liu G.J Aeronaut Mater,2006;26(3):83(李峰,苑世剑,刘钢.航空材料学报,2006;26(3):83)
[11]Wang Z R.J Mater Proc Technol,1995;55:1
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!