| THE RESEACH ON METAL FLOW DURING EXTRUDING PROCESS UNDER DIFFERENT FRICTION CONDITIONS BY DEFORMING AREA DIVISIO |
| LI Feng |
| 哈尔滨工业大学 |
|
Cite this article:
LI Feng. THE RESEACH ON METAL FLOW DURING EXTRUDING PROCESS UNDER DIFFERENT FRICTION CONDITIONS BY DEFORMING AREA DIVISIO. Acta Metall Sin, 2007, 43(2): 199-204 .
|
|
|
Abstract In order to investigate the metal flow behavior during extrusion process with active friction, numerical simulations and experiments were employed to investigate the mechanical mechanism of the extrusion process with active friction. The characteristic quantity such as the second invariant of the deviatoric stress tensor (J2)、Lode parameter( ) were employed for the division of deformation area. The results show that when extruding with active friction, no metal flow interface forms at the container bottom, the dead metal zone completely disappears, the deformation type of the metal in the plastic deformation area changes from three to the tension type, and the homogeneity of the deformation as well as metal flow is greatly improved. Therefore, it will be easy for extruding and promoting the extrudates quality.
|
|
Received: 05 June 2006
|
|
|
[1]Shan D B,Xu W C,Lu Y.J Mater Process Technol,2004;151:289 [2]Hsu T C,Huang C C.J Mater Process Technol,2003;140:49 [3]Tan X C.Int Tribol,2002;35:385 [4]Lin Z P,Hua J.J Nanchang Univ,1988;10(1):20(林治平,花江.南昌大学学报.1988;10(1):20) [5]Miiller K B.In:Kiuchi M,Nishimura H,Yanagimoto J,eds.,Advanced Technology of Plasticity 2002,Pvoc 7th ICTP,Japan,2002:427 [6]He Z B,Hu W L,Wang Z R.In:Bariani P Fed,Advanced Technology of Plasticity 2005,Proc 8th ICTP,Verona,Italy:Edizioni Progetto Padova,2005:407 [7]Wang Z R.Fundamental of Plastic Working Mechanics.Beijing:National Defence Industry Press,1989:127(王仲仁.塑性加工力学基础.北京:国防工业出版社,1989:127) [8]Hu W L,He Z B,Fang Y.J Mater Process Technol,2004;151:27 [9]He Z B.PhD Dissertation,Harbin Institute of Technology,2005(何祝斌.哈尔滨工业大学博士学位论文,2005) [10]Li F,Yuan S J,Liu G.J Aeronaut Mater,2006;26(3):83(李峰,苑世剑,刘钢.航空材料学报,2006;26(3):83) [11]Wang Z R.J Mater Proc Technol,1995;55:1 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|