| SIMULATION OF TEMPERATURE FIELD DURING HIGH-FREQUENCY RESISTANCE HEATING-ROLLING COMPOSITE STRIP |
| XIAO Nan; CHEN Haigeng;SUN Shigang; WANG Chengjun; CUI Miao;YU Jiuming |
| 东北大学材料与冶金学院 |
|
Cite this article:
XIAO Nan; CHEN Haigeng; SUN Shigang; WANG Chengjun; CUI Miao; YU Jiuming. SIMULATION OF TEMPERATURE FIELD DURING HIGH-FREQUENCY RESISTANCE HEATING-ROLLING COMPOSITE STRIP. Acta Metall Sin, 2006, 42(9): 989-992 .
|
|
|
Abstract The dynamic temperature field during roll-bonding combined with high-frequency alternating current heating has been numerically simulated by a simplified model. In the simplified model, the governing equation of heat conduction is discretized
using implicit finite difference method, and the computational domain is discretized using cell centered scheme, and the solution of Maxwell equation is used to determine the distribution of the internal heating sources. Considering the saltation of magnetic permeability of the ferromagnetic material when its temperature is more than the Curie point, the general solution of Maxwell equation is deduced. Based on our new method three kinds of composite strips (steel-Al, steel-Cu, steel-stainless steel) are performed numerically to validate the feasibility of the combination of various technical parameters.
|
|
Received: 23 December 2005
|
| ZTFLH: |
TB331
|
|
| |
TK124
|
|
| |
TM154.22
|
|
|
[1]Carreon M A,Guliants V V.Catal Today,2005;99:137 [2]Murakami Y,Esumi K,Honda H.Carbon,1996;34:463 [3]Huang L Z.The Principle of Electromagnetic Field.Shanghai:People's Education Press,1980:307(黄礼镇.电磁场原理.上海:人民教育出版社,1980:307) [4]Ni G Z.The Principle of Engineering Electromagnetic Field.Beijing:Higher Education Press,2002:190(倪光正.工程电磁场原理.北京:高等教育出版社,2002:190) [5]Zu G Y,Yu J M,Wen J L.Res Iron Steel,2004;(1):30(祖国胤,于九明,温景林.钢铁研究,2004;(1):30) [6]Devyatko Y N,Rogozhkin S V.Vacuum,2002;66:123 [7]Macdonald J R,Ausloos M.Physica,1997;242A:150 [8]Tao W Q.Numerical Heat Transfer.Xi'an:Xi'an Jiaotong University Press,1988:11(陶文铨.数值传热学.西安:西安交通大学出版社,1988:11) [9]Croft D R,Lilley D G.Heat Transfer Calculations Using Finite Difference Equations.London:Applied Science Publishers Ltd.,1977:139 [10]Kim I S,Basu A.J Mater Process Technol,1998;77:17 [11]Fu X,Yu J M,Chen H G.Acts Metall Sin,2000;36:828(傅晓,于九明,陈海耿.金属学报,2000;36:828) [12]Xu Z B,Zhu Z Y,Wang W J,Zhang J M,Wang L F.J Iron Steel Res,1999;11(1):12(许中波,朱志远,王万军,张炯明,王立峰.钢铁研究学报,1999;11(1):12) [13]Zhao X H.The Pressure Welds.Beijing:China Machine Press,1998:191(赵熹华.压力焊.北京:机械工业出版社,1988:191) [14]Little G H,Kamtekar A G.Comput Struct,1998;68:157 [15]Miller M K,Babu S S,Sokolov M A,Nanstad R K,Iskander S K.Mater Sci Eng,2002;A327:76L |