| CALCULATION AND DISCUSSION ON THE HEAT FLUX IN MOULD OF CONTINUOUS CASTING ROUND BILLET |
| GUO Liangliang; YAO Man; YIN Hebi; WANG Xudong; FANG Dacheng;LIU Xiao; YU Yan |
| 大连理工大学材料科学与工程学院 |
|
Cite this article:
GUO Liangliang; YAO Man; YIN Hebi; WANG Xudong; FANG Dacheng; LIU Xiao; YU Yan. CALCULATION AND DISCUSSION ON THE HEAT FLUX IN MOULD OF CONTINUOUS CASTING ROUND BILLET. Acta Metall Sin, 2006, 42(9): 983-988 .
|
|
|
Abstract Based on the measured data of mould temperatures and heat flux, an inverse problem of mathematic model was developed to calculate the field of heat flux for continuous casting round billet. The characteristics of non-uniform longitudinal and circumferential heat fluxes were shown explicitly. The calculated formulae of longitudinal and circumferential heat fluxes were obtained by fitting the calculated
heat flux with considering the effect of casting speeds and mould installation statuses and were compared with the published experiential formulae. The inverse problem simulation and the fitted heat flux formulae are helpful for visualization of mould process and analysis of heat flux and accident in continuous casting round billet.
|
|
Received: 09 December 2005
|
|
|
[1]Alvarez de Toledo G,Ciriza J,Laraudogoitia J J.Ironmaking Steelmaking,2003;30:360 [2]Yao M,Yin H B.Ironmaking Steelmaking,2005;32:359 [3]Billany T J H,Normanton A S,Mills K C.Ironmaking Steelmaking,1991;18:403 [4]Irving W R,Perkins A.Ironmaking Steelmaking,1977;4:292 [5]Ikeda M,Asabim K,Nakano T.Trans Iron Steel Inst Jpn,1981;21B:511 [6]Mills K C,Billany T J H,Normanton A S.Ironmaking Steelmaking,1991;18:253 [7]Zhang J M,Zhang L,Wang X H,Wang L F.Acta Metall Sin,2003;39:1285(张炯明,张立,王新华,王立峰.金属学报,2003;39:1285) [8]Zhang X Z,Na X Z,Wang Z Y,Liu A Q,Gan Y.Acta Metall Sin,2004;40:281(张兴中,那贤昭,王忠英,刘爱强,干勇.金属学报,2004;40:281) [9]Pinheiro C A M,Samarasekera I V Brimacombe J K,Walker B N.Ironmaking Steelmaking,2000;27:37 [10]Chow C,Samarasekera I V,Walker B N,Lockhart G.Ironmaking Steelmaking,2002;29:61 [11]Yao M,Yin H B,Fang D C.ISIJ Int,2004;44:1696 [12]Savage J,Pritchard W H.Iron Steel Inst London,1954;11:260 [13]Yang H L,Zhao L G.Metall Mater Trans,1998;29B:1345 [14]Chow C,Samarasekera I V.Ironmaking Steelmaking,2002;29:53b |