PATTERNS OF CELL DEATH INDUCED BY FERRITE STAINLESS STEEL OF MAGNETIC ATTACHMENT IN THE MOUSE FIBROBLAST L929 CELLS
中国医科大学口腔医学院
Cite this article: 

. PATTERNS OF CELL DEATH INDUCED BY FERRITE STAINLESS STEEL OF MAGNETIC ATTACHMENT IN THE MOUSE FIBROBLAST L929 CELLS. Acta Metall Sin, 2006, 42(8): 892-896 .

Download:  PDF(1140KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The magnetic attachment wrapped with 26-1 ultra-purified ferrite stainless steel can improve its corrosion resistance. The fibroblast L929 cells of mouse were treated in vitro through 3 kinds of leaching liquors of stainless steel to detect the apoptosis rate and cell cycle distribution of L929 by the flow cytometry PI staining method, and the morphology of cell apoptosis was observed by electron microscope. Compared with the Tilite alloy and Co-Cr alloy, the type of cell apoptosis was quantitatively determined by di-parameter technique in which the annexin was marked by the fluorescein isothiocyanate (FIT) and stained by the iodonadine. The result showed that 26-1 ferrite stainless steel can induce the apoptosis of L929 cells with a fashion of time-dependence, and the apoptosis rate depends on the concentration of the leaching liquor. It also proved that 26-1 ferrite stainless steel meets the biocompatibility as a clinical material and can be safely applied in clinic.
Key words:       
Received:  24 February 2006     
ZTFLH:  R783.1  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I8/892

[1]Matsumura H,Kawasaki K.J Prosthet Dent,2000;84:22
[2]Watanba I,Tanaka Y,Ohkubo C.Amp W M.J Prosthet Dent,2002;88:573
[3]Wilson M,Kpendema H,Noar J H.J Biomater,1995;16:721
[4]Thean H P,Khor S K,Loh P L.J Quintessence Int,2001;32:517
[5]David A,Lober D.Eur J Orthod,2004;26:421
[6]Al-Hiyasat A S,Bashahsheh O M,Darmani H.Int J Prothodont,2003;16:8
[7]Al-Hiyasat A S,Darmani H,Bashabsheh O M.Int J Prothodont,2003;16:597
[8]Majno G,Joris I.Am J Pathol,1995;146,3
[9]Fabre T,Belloc F,Dupuy B.J Biomed Mater Res,1999;44,429
[10]Kapanen A,Ilvesaro J,Danilov A,Ryhanen J,Lehenkari P,Tunkaene J.J Biomater,2002;23:645
[11]Chen Y B,Hou J,Fu W N,Ding S Q,Wang D X,Yuan Z G,Kong X T.J Cancer,2003;22:1276(陈玉宝,侯健,傅卫年,丁思奇,王东星,袁振刚,孔宪涛.癌症,2003;22:1276)
[12]Vermes I,Haanen C,Steffens-Nakken H.J Lmmunol Methods,1995;184:39
[13]van Engeland M,Nieland L J W,Ramaekers F C S,Schutte B,Reutelingsperger C P M.J Cytometry,1998;31:1
[14]Span L F R,Pennings A H M,Vierwinden G.J Cytometry,2002;47:24
[15]Lefebvre C A,Schuster G S,Marr J C.Int J Prothodont,1995;8:122
[16]Richardson R R Jr,Miller J A,Reicher W M.J Biomater,1993;14:627
[17]Zhan D S,Qi L,Zhu J T,Bai B,Jiang G F.Chin J Hemorheology,2005;15:39(战德松,戚琳,朱静涛,白冰,姜国锋.中国血液流变学杂志,2005;15:39)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!